Twice cold reduced tin plate and manufacture method thereof

The invention discloses a twice cold reduced tin plate and a manufacture method thereof, belonging to the technical field of steel rolling. Chemical components of the twice cold reduced tint plate comprise 0.06%-0.09% of C, less than or equal to 0.02% of Si, 0.30%-0.50% of Mn, less than or equal to...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SONG HAO, SUN CHAOFAN, LIU WEI, SHI YUNGUANG, ZHANG ZHAO'EN, ZHU FANGXIU, WANG YAQING, MO ZHIYING, CUI YANG, HUANG XUEQI, ZHOU JIMING, FANG YUAN, WU ZHIGUO, YIN XIANDONG, ZHANG BAOLAI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses a twice cold reduced tin plate and a manufacture method thereof, belonging to the technical field of steel rolling. Chemical components of the twice cold reduced tint plate comprise 0.06%-0.09% of C, less than or equal to 0.02% of Si, 0.30%-0.50% of Mn, less than or equal to 0.015% of P, less than or equal to 0.012% of S, 0.005%-0.02% of Als, 0.0200%-0.0250% of N, and the balance of Fe and inevitable impurities. The manufacture method comprises the steps of continuous casting, hot rolling, acid pickling, cold rolling, continuous annealing, secondary cold rolling, and tin plating. Due to component proportioning and process optimization, the prepared tin plate is low-cost but has high strength and high plasticity. 本发明公开了种二次冷轧镀锡板及其生产方法,属于轧钢技术领域。按照质量百分比,所述二次冷轧镀锡板的化学成分为:C:0.06%~0.09%,Si≤0.02%,Mn:0.30%~0.50%,P≤0.015%,S≤0.012%,Als:0.005%~0.02%,N:0.0200%~0.0250%,余量为Fe及不可避免的杂质。其生产方法包括连铸、热轧、酸洗、冷轧、连续退火、二次冷轧及镀锡过程。本发明通过成分设计和工艺优化,可生产低成本、高强度、高塑性的镀锡板。