Strength delayed concrete and application thereof to A/B occlusive piles

The invention provides strength delayed concrete and an application thereof in A/B occlusive piles. In terms of dosage per cubic meter, the strength delayed concrete is prepared from components as follows: 150-350 kg of cement, 180-190 kg of water, 600-900 kg of sand, 1100-1250 kg of pebbles, 50-100...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HUANG XINGXIANG, WANG JUJIN, TANG SHITAO, PAN HONGDE, HU CHANGWU, WEI JIABIN, XI YUXIN, ZHAI WENJIA, LIU SHENGQIU, QIN XIANGRONG, XIE YONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention provides strength delayed concrete and an application thereof in A/B occlusive piles. In terms of dosage per cubic meter, the strength delayed concrete is prepared from components as follows: 150-350 kg of cement, 180-190 kg of water, 600-900 kg of sand, 1100-1250 kg of pebbles, 50-100 kg of an admixture and 3-7 kg of a retarder. The strength of the strength delayed concrete is increased slowly at the early stage, 7d strength is just 30%-50% of designed strength value under the natural curing condition, 28d strength can reach 100% or higher of the designed strength value, workability is good, and pouring is compacter. With application of the strength delayed concrete to the A/B occlusive piles, a pile A can be subjected to rotary excavating and cutting smoothly, and requirements of the pile A for soil blocking and water stopping can be met. 本发明提供了种缓强混凝土及其在A/B咬合桩中的应用。本发明提供的缓强混凝土以单方用量计,包括以下含量的组分:水泥150~350kg;水180~190kg;砂600~900kg;石子1100~1250kg;掺合料50~100kg;缓凝剂3~7kg。本发明提供的缓强混凝土在初期强度增长缓慢,在自然养护条件下,7d强度