Non-sparking wear-resisting concrete and method for carrying out floor construction through concrete
The invention discloses non-sparking wear-resisting concrete and a method for carrying out floor construction through the concrete. The non-sparking wear-resisting concrete is prepared from, by weight, 3.42-4.45 parts of conductive powder, 0.5-2.5 parts of common sand, 3.2-4.88 parts of coarse aggre...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention discloses non-sparking wear-resisting concrete and a method for carrying out floor construction through the concrete. The non-sparking wear-resisting concrete is prepared from, by weight, 3.42-4.45 parts of conductive powder, 0.5-2.5 parts of common sand, 3.2-4.88 parts of coarse aggregate, 2-2.2 parts of SBS high polymer modified emulsified asphalt, 0.5-1.2 parts of cement, 1 part of water and 0.4-0.8 part of an additive. The additive is a combination of one or more of a fire retardant, a wear resisting agent, a foaming agent, a carbon forming agent, a carbon catalyst, a water reducing agent and a pumping agent. The conductive powder is a combination of one or more of spherical silicon-based conductive powder, electric mica powder, conductive titanium dioxide and conductive barium sulfate. The non-sparking wear-resisting concrete can be widely applied to ground construction of combustible product warehouses, production areas with sparks prone to being generated or explosive plants, hangars and |
---|