Maritime work portland cement and preparation method thereof

The invention relates to maritime work portland cement and a preparation method thereof. The maritime work portland cement comprises the following components in percentage by mass: 18%-50% of clinker, 30%-60% of common mineral powder, 5%-15% of superfine mineral powder, 0%-20% of pulverized fuel ash...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DENG KAI, LIU XIANGYANG, WEI HUAIJUN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DENG KAI
LIU XIANGYANG
WEI HUAIJUN
description The invention relates to maritime work portland cement and a preparation method thereof. The maritime work portland cement comprises the following components in percentage by mass: 18%-50% of clinker, 30%-60% of common mineral powder, 5%-15% of superfine mineral powder, 0%-20% of pulverized fuel ash and 8%-12% of gypsum. The maritime work portland cement has excellent chloride ion erosion resistance and excellent mechanical performance; the maximum permeability coefficient of chloride ions in the 28d portland cement can reach 0.36*10 m /s; and the compressive strength of the 28d portent cement can exceed 55MPa, and therefore, the maritime work portland cement is particularly suitable for preparing concrete with high strength, high permeability resistance and high erosion resistance for ocean engineering. 本发明涉及种海工硅酸盐水泥及其制备方法,所述海工硅酸盐水泥,包括如下质量百分比的组分:熟料18%-50%、普通矿粉30%-60%、超细矿粉5%-15%、粉煤灰0%-20%、石膏8%-12%。上述海工硅酸盐水泥具有优异的抗氯离子侵蚀性能及力学性能,28d氯离子渗透系数最低可达0.36×10m/s,而且28d抗压强度可超过55MPa,特别适合配制高强、高抗渗和高抗侵蚀的海洋工程用混凝土。
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN106431036A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN106431036A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN106431036A3</originalsourceid><addsrcrecordid>eNrjZLDxTSzKLMnMTVUozy_KVijILyrJScxLUUhOzU3NK1EAMQuKUgsSixJLMvPzFHJTSzLyUxRKMlKLUvPTeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoYGZibGhgbGZozExagAOKjAU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Maritime work portland cement and preparation method thereof</title><source>esp@cenet</source><creator>DENG KAI ; LIU XIANGYANG ; WEI HUAIJUN</creator><creatorcontrib>DENG KAI ; LIU XIANGYANG ; WEI HUAIJUN</creatorcontrib><description>The invention relates to maritime work portland cement and a preparation method thereof. The maritime work portland cement comprises the following components in percentage by mass: 18%-50% of clinker, 30%-60% of common mineral powder, 5%-15% of superfine mineral powder, 0%-20% of pulverized fuel ash and 8%-12% of gypsum. The maritime work portland cement has excellent chloride ion erosion resistance and excellent mechanical performance; the maximum permeability coefficient of chloride ions in the 28d portland cement can reach 0.36*10 m /s; and the compressive strength of the 28d portent cement can exceed 55MPa, and therefore, the maritime work portland cement is particularly suitable for preparing concrete with high strength, high permeability resistance and high erosion resistance for ocean engineering. 本发明涉及种海工硅酸盐水泥及其制备方法,所述海工硅酸盐水泥,包括如下质量百分比的组分:熟料18%-50%、普通矿粉30%-60%、超细矿粉5%-15%、粉煤灰0%-20%、石膏8%-12%。上述海工硅酸盐水泥具有优异的抗氯离子侵蚀性能及力学性能,28d氯离子渗透系数最低可达0.36×10m/s,而且28d抗压强度可超过55MPa,特别适合配制高强、高抗渗和高抗侵蚀的海洋工程用混凝土。</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170222&amp;DB=EPODOC&amp;CC=CN&amp;NR=106431036A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170222&amp;DB=EPODOC&amp;CC=CN&amp;NR=106431036A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DENG KAI</creatorcontrib><creatorcontrib>LIU XIANGYANG</creatorcontrib><creatorcontrib>WEI HUAIJUN</creatorcontrib><title>Maritime work portland cement and preparation method thereof</title><description>The invention relates to maritime work portland cement and a preparation method thereof. The maritime work portland cement comprises the following components in percentage by mass: 18%-50% of clinker, 30%-60% of common mineral powder, 5%-15% of superfine mineral powder, 0%-20% of pulverized fuel ash and 8%-12% of gypsum. The maritime work portland cement has excellent chloride ion erosion resistance and excellent mechanical performance; the maximum permeability coefficient of chloride ions in the 28d portland cement can reach 0.36*10 m /s; and the compressive strength of the 28d portent cement can exceed 55MPa, and therefore, the maritime work portland cement is particularly suitable for preparing concrete with high strength, high permeability resistance and high erosion resistance for ocean engineering. 本发明涉及种海工硅酸盐水泥及其制备方法,所述海工硅酸盐水泥,包括如下质量百分比的组分:熟料18%-50%、普通矿粉30%-60%、超细矿粉5%-15%、粉煤灰0%-20%、石膏8%-12%。上述海工硅酸盐水泥具有优异的抗氯离子侵蚀性能及力学性能,28d氯离子渗透系数最低可达0.36×10m/s,而且28d抗压强度可超过55MPa,特别适合配制高强、高抗渗和高抗侵蚀的海洋工程用混凝土。</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDxTSzKLMnMTVUozy_KVijILyrJScxLUUhOzU3NK1EAMQuKUgsSixJLMvPzFHJTSzLyUxRKMlKLUvPTeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoYGZibGhgbGZozExagAOKjAU</recordid><startdate>20170222</startdate><enddate>20170222</enddate><creator>DENG KAI</creator><creator>LIU XIANGYANG</creator><creator>WEI HUAIJUN</creator><scope>EVB</scope></search><sort><creationdate>20170222</creationdate><title>Maritime work portland cement and preparation method thereof</title><author>DENG KAI ; LIU XIANGYANG ; WEI HUAIJUN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN106431036A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2017</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>DENG KAI</creatorcontrib><creatorcontrib>LIU XIANGYANG</creatorcontrib><creatorcontrib>WEI HUAIJUN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DENG KAI</au><au>LIU XIANGYANG</au><au>WEI HUAIJUN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Maritime work portland cement and preparation method thereof</title><date>2017-02-22</date><risdate>2017</risdate><abstract>The invention relates to maritime work portland cement and a preparation method thereof. The maritime work portland cement comprises the following components in percentage by mass: 18%-50% of clinker, 30%-60% of common mineral powder, 5%-15% of superfine mineral powder, 0%-20% of pulverized fuel ash and 8%-12% of gypsum. The maritime work portland cement has excellent chloride ion erosion resistance and excellent mechanical performance; the maximum permeability coefficient of chloride ions in the 28d portland cement can reach 0.36*10 m /s; and the compressive strength of the 28d portent cement can exceed 55MPa, and therefore, the maritime work portland cement is particularly suitable for preparing concrete with high strength, high permeability resistance and high erosion resistance for ocean engineering. 本发明涉及种海工硅酸盐水泥及其制备方法,所述海工硅酸盐水泥,包括如下质量百分比的组分:熟料18%-50%、普通矿粉30%-60%、超细矿粉5%-15%、粉煤灰0%-20%、石膏8%-12%。上述海工硅酸盐水泥具有优异的抗氯离子侵蚀性能及力学性能,28d氯离子渗透系数最低可达0.36×10m/s,而且28d抗压强度可超过55MPa,特别适合配制高强、高抗渗和高抗侵蚀的海洋工程用混凝土。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN106431036A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Maritime work portland cement and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T04%3A48%3A09IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DENG%20KAI&rft.date=2017-02-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN106431036A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true