Chrome-molybdenum-copper abrasion-resistant cast iron and preparation method thereof

The invention discloses chrome-molybdenum-copper abrasion-resistant cast iron and a preparation method thereof. The chrome-molybdenum-copper abrasion-resistant cast iron comprises the components of, by weight, 2.8%-3.8% of C, 1.65%-2.7% of Si, 0.5%-1.2% of Mn, 0.12%-0.7% of P, 0.2%-0.5% of Cr, 0.3%-...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: ZHOU BINGZHEN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses chrome-molybdenum-copper abrasion-resistant cast iron and a preparation method thereof. The chrome-molybdenum-copper abrasion-resistant cast iron comprises the components of, by weight, 2.8%-3.8% of C, 1.65%-2.7% of Si, 0.5%-1.2% of Mn, 0.12%-0.7% of P, 0.2%-0.5% of Cr, 0.3%-0.8% of Mo, 0.55%-1.4% of Cu, 0-0.09% of S, and the balance Fe. The preparation method comprises the steps of burdening, preheating, smelting, on-the-spot sample quick analysis, final deoxidation, inoculation treatment and pouring. According to the preparation method, the casting process is simple, the structure is refined significantly, the mechanical strength, abrasion resistance, heat resistance and other comprehensive properties are improved, the mechanical property can reach the HT250 grade, and the casting process is especially suitable for casting cylinders, piston rings and tappets. 本发明公开了种铬钼铜耐磨铸铁及其制备方法,所述的铬钼铜耐磨铸铁其成分的重量百分比为C2.8~3.8%、Si1.65~2.7%、Mn0.5~1.2%、P0.12~0.7%、Cr0.2~0.5%、Mo0.3~0.8%、Cu0.55~1.4%、S≤0.09%