Method for determining acidolysis rate of titanium slag
The invention discloses a method for determining acidolysis rate of titanium slag. The method comprises the steps of (1) Levigating the titanium slag to obtain powder of titanium slag; (2) Mixing the powder of titanium slag with oil of vitriol and completing acidolysis to obtain acid solution and su...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | ZHANG YUN CHEN HEFEN YANG HAO PENG DONGHUI LI XIYU ZHANG JIAN YAO DONGYAN CHEN LINGXIAN XU FUCHANG YANG LIHUA DUAN QINGYUE SHEN SHAOKUN |
description | The invention discloses a method for determining acidolysis rate of titanium slag. The method comprises the steps of (1) Levigating the titanium slag to obtain powder of titanium slag; (2) Mixing the powder of titanium slag with oil of vitriol and completing acidolysis to obtain acid solution and sulfur dioxide; (3) Curing the acid solution to obtain cured solution and sulfur dioxide; (4) Performing leaching-filtration treatment for the cured solution to obtain titanium containing filtrate and filter residue; (5) Reducing the titanium containing filtrate to obtain titanium containing filtrate; (6) Performing titration for the titanium containing filtrate with the standard solution of ammonium ferric sulfate and recording the volume of the ammonium ferric sulfate V1; (7) Ashing the filter residue and dissolving to obtain the solution; (8) Reducing the solution to obtain titanium containing solution; (9) Performing titration for the titanium containing filtrate with the standard solution of ammonium ferric sulf |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN106324184A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN106324184A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN106324184A3</originalsourceid><addsrcrecordid>eNrjZDD3TS3JyE9RSMsvUkhJLUktys3My8xLV0hMzkzJz6kszixWKEosSVXIT1MoySxJzMsszVUozklM52FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hgZmxkYmhhYmjsbEqAEA3gQt_Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for determining acidolysis rate of titanium slag</title><source>esp@cenet</source><creator>ZHANG YUN ; CHEN HEFEN ; YANG HAO ; PENG DONGHUI ; LI XIYU ; ZHANG JIAN ; YAO DONGYAN ; CHEN LINGXIAN ; XU FUCHANG ; YANG LIHUA ; DUAN QINGYUE ; SHEN SHAOKUN</creator><creatorcontrib>ZHANG YUN ; CHEN HEFEN ; YANG HAO ; PENG DONGHUI ; LI XIYU ; ZHANG JIAN ; YAO DONGYAN ; CHEN LINGXIAN ; XU FUCHANG ; YANG LIHUA ; DUAN QINGYUE ; SHEN SHAOKUN</creatorcontrib><description>The invention discloses a method for determining acidolysis rate of titanium slag. The method comprises the steps of (1) Levigating the titanium slag to obtain powder of titanium slag; (2) Mixing the powder of titanium slag with oil of vitriol and completing acidolysis to obtain acid solution and sulfur dioxide; (3) Curing the acid solution to obtain cured solution and sulfur dioxide; (4) Performing leaching-filtration treatment for the cured solution to obtain titanium containing filtrate and filter residue; (5) Reducing the titanium containing filtrate to obtain titanium containing filtrate; (6) Performing titration for the titanium containing filtrate with the standard solution of ammonium ferric sulfate and recording the volume of the ammonium ferric sulfate V1; (7) Ashing the filter residue and dissolving to obtain the solution; (8) Reducing the solution to obtain titanium containing solution; (9) Performing titration for the titanium containing filtrate with the standard solution of ammonium ferric sulf</description><language>chi ; eng</language><subject>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES ; MEASURING ; PHYSICS ; TESTING</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20170111&DB=EPODOC&CC=CN&NR=106324184A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20170111&DB=EPODOC&CC=CN&NR=106324184A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG YUN</creatorcontrib><creatorcontrib>CHEN HEFEN</creatorcontrib><creatorcontrib>YANG HAO</creatorcontrib><creatorcontrib>PENG DONGHUI</creatorcontrib><creatorcontrib>LI XIYU</creatorcontrib><creatorcontrib>ZHANG JIAN</creatorcontrib><creatorcontrib>YAO DONGYAN</creatorcontrib><creatorcontrib>CHEN LINGXIAN</creatorcontrib><creatorcontrib>XU FUCHANG</creatorcontrib><creatorcontrib>YANG LIHUA</creatorcontrib><creatorcontrib>DUAN QINGYUE</creatorcontrib><creatorcontrib>SHEN SHAOKUN</creatorcontrib><title>Method for determining acidolysis rate of titanium slag</title><description>The invention discloses a method for determining acidolysis rate of titanium slag. The method comprises the steps of (1) Levigating the titanium slag to obtain powder of titanium slag; (2) Mixing the powder of titanium slag with oil of vitriol and completing acidolysis to obtain acid solution and sulfur dioxide; (3) Curing the acid solution to obtain cured solution and sulfur dioxide; (4) Performing leaching-filtration treatment for the cured solution to obtain titanium containing filtrate and filter residue; (5) Reducing the titanium containing filtrate to obtain titanium containing filtrate; (6) Performing titration for the titanium containing filtrate with the standard solution of ammonium ferric sulfate and recording the volume of the ammonium ferric sulfate V1; (7) Ashing the filter residue and dissolving to obtain the solution; (8) Reducing the solution to obtain titanium containing solution; (9) Performing titration for the titanium containing filtrate with the standard solution of ammonium ferric sulf</description><subject>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES</subject><subject>MEASURING</subject><subject>PHYSICS</subject><subject>TESTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD3TS3JyE9RSMsvUkhJLUktys3My8xLV0hMzkzJz6kszixWKEosSVXIT1MoySxJzMsszVUozklM52FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hgZmxkYmhhYmjsbEqAEA3gQt_Q</recordid><startdate>20170111</startdate><enddate>20170111</enddate><creator>ZHANG YUN</creator><creator>CHEN HEFEN</creator><creator>YANG HAO</creator><creator>PENG DONGHUI</creator><creator>LI XIYU</creator><creator>ZHANG JIAN</creator><creator>YAO DONGYAN</creator><creator>CHEN LINGXIAN</creator><creator>XU FUCHANG</creator><creator>YANG LIHUA</creator><creator>DUAN QINGYUE</creator><creator>SHEN SHAOKUN</creator><scope>EVB</scope></search><sort><creationdate>20170111</creationdate><title>Method for determining acidolysis rate of titanium slag</title><author>ZHANG YUN ; CHEN HEFEN ; YANG HAO ; PENG DONGHUI ; LI XIYU ; ZHANG JIAN ; YAO DONGYAN ; CHEN LINGXIAN ; XU FUCHANG ; YANG LIHUA ; DUAN QINGYUE ; SHEN SHAOKUN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN106324184A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2017</creationdate><topic>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES</topic><topic>MEASURING</topic><topic>PHYSICS</topic><topic>TESTING</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG YUN</creatorcontrib><creatorcontrib>CHEN HEFEN</creatorcontrib><creatorcontrib>YANG HAO</creatorcontrib><creatorcontrib>PENG DONGHUI</creatorcontrib><creatorcontrib>LI XIYU</creatorcontrib><creatorcontrib>ZHANG JIAN</creatorcontrib><creatorcontrib>YAO DONGYAN</creatorcontrib><creatorcontrib>CHEN LINGXIAN</creatorcontrib><creatorcontrib>XU FUCHANG</creatorcontrib><creatorcontrib>YANG LIHUA</creatorcontrib><creatorcontrib>DUAN QINGYUE</creatorcontrib><creatorcontrib>SHEN SHAOKUN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG YUN</au><au>CHEN HEFEN</au><au>YANG HAO</au><au>PENG DONGHUI</au><au>LI XIYU</au><au>ZHANG JIAN</au><au>YAO DONGYAN</au><au>CHEN LINGXIAN</au><au>XU FUCHANG</au><au>YANG LIHUA</au><au>DUAN QINGYUE</au><au>SHEN SHAOKUN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for determining acidolysis rate of titanium slag</title><date>2017-01-11</date><risdate>2017</risdate><abstract>The invention discloses a method for determining acidolysis rate of titanium slag. The method comprises the steps of (1) Levigating the titanium slag to obtain powder of titanium slag; (2) Mixing the powder of titanium slag with oil of vitriol and completing acidolysis to obtain acid solution and sulfur dioxide; (3) Curing the acid solution to obtain cured solution and sulfur dioxide; (4) Performing leaching-filtration treatment for the cured solution to obtain titanium containing filtrate and filter residue; (5) Reducing the titanium containing filtrate to obtain titanium containing filtrate; (6) Performing titration for the titanium containing filtrate with the standard solution of ammonium ferric sulfate and recording the volume of the ammonium ferric sulfate V1; (7) Ashing the filter residue and dissolving to obtain the solution; (8) Reducing the solution to obtain titanium containing solution; (9) Performing titration for the titanium containing filtrate with the standard solution of ammonium ferric sulf</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN106324184A |
source | esp@cenet |
subjects | INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES MEASURING PHYSICS TESTING |
title | Method for determining acidolysis rate of titanium slag |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T05%3A36%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20YUN&rft.date=2017-01-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN106324184A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |