Titanium microalloy strengthened pipeline steel hot-rolled coiled plate and production method thereof

The invention relates to the technical field of steel materials, in particular to a titanium microalloy strengthened pipeline steel hot-rolled coiled plate and a production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate. The production method of the titanium mi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GUAN LIUHUI, LI YONG, WEI XIAN, GUO SHIBAO, CHENG GUANJIANG, ZHOU MAOQI, WEI YUZHI, PEI FENGJUAN, ZHANG LINGZHI, XU DANGWEI, BAI JINHAN, WANG CHAOHAI, LI JINGYU, PAN SONGJUN, WANG XIANGSONG, LIU HAIQIANG, RAO JING, KONG DENAN, WANG XINJIANG, MAO JINHUA, SHANG CUNLIANG, CHEN DONGZHI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GUAN LIUHUI
LI YONG
WEI XIAN
GUO SHIBAO
CHENG GUANJIANG
ZHOU MAOQI
WEI YUZHI
PEI FENGJUAN
ZHANG LINGZHI
XU DANGWEI
BAI JINHAN
WANG CHAOHAI
LI JINGYU
PAN SONGJUN
WANG XIANGSONG
LIU HAIQIANG
RAO JING
KONG DENAN
WANG XINJIANG
MAO JINHUA
SHANG CUNLIANG
CHEN DONGZHI
description The invention relates to the technical field of steel materials, in particular to a titanium microalloy strengthened pipeline steel hot-rolled coiled plate and a production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate comprises the working procedures of pretreatment of molten iron, top-bottom combined blowing converter processing, LF refining, double-strand slab continuous casting, steel rolling carried out through a hot continuous rolling mill, laminar cooling and coiling. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate is characterized in that during LF refining, the tapping temperature is 1630-1690 DEG C, and the steel smelting components are controlled to include, by weight, 0.06%-0.09% of C, 0.80%-1.50% of Mn, 0.10%-0.30% of Si, not larger than 0.010% of S, not larger than 0.025% of P, 0.035%-0.060% of Ti, not l
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN106319352A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN106319352A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN106319352A3</originalsourceid><addsrcrecordid>eNqNjbEKwkAQRNNYiPoP6wcEjEHBUoJiZZU-HJeJWdjcHpdN4d97gh9g9YaZYWZdoGVzgZeJJvZJnYi-abaE8LIRAT1FjhAOyC4gNKqVSUVy4pW_iOIM5EJWSfvFG2ugCTZqT3kjQYdtsRqczNj9uCn291vbPEpE7TBH5_OVdc2zOpzr6lKfjtf6n84HtLdAFA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Titanium microalloy strengthened pipeline steel hot-rolled coiled plate and production method thereof</title><source>esp@cenet</source><creator>GUAN LIUHUI ; LI YONG ; WEI XIAN ; GUO SHIBAO ; CHENG GUANJIANG ; ZHOU MAOQI ; WEI YUZHI ; PEI FENGJUAN ; ZHANG LINGZHI ; XU DANGWEI ; BAI JINHAN ; WANG CHAOHAI ; LI JINGYU ; PAN SONGJUN ; WANG XIANGSONG ; LIU HAIQIANG ; RAO JING ; KONG DENAN ; WANG XINJIANG ; MAO JINHUA ; SHANG CUNLIANG ; CHEN DONGZHI</creator><creatorcontrib>GUAN LIUHUI ; LI YONG ; WEI XIAN ; GUO SHIBAO ; CHENG GUANJIANG ; ZHOU MAOQI ; WEI YUZHI ; PEI FENGJUAN ; ZHANG LINGZHI ; XU DANGWEI ; BAI JINHAN ; WANG CHAOHAI ; LI JINGYU ; PAN SONGJUN ; WANG XIANGSONG ; LIU HAIQIANG ; RAO JING ; KONG DENAN ; WANG XINJIANG ; MAO JINHUA ; SHANG CUNLIANG ; CHEN DONGZHI</creatorcontrib><description>The invention relates to the technical field of steel materials, in particular to a titanium microalloy strengthened pipeline steel hot-rolled coiled plate and a production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate comprises the working procedures of pretreatment of molten iron, top-bottom combined blowing converter processing, LF refining, double-strand slab continuous casting, steel rolling carried out through a hot continuous rolling mill, laminar cooling and coiling. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate is characterized in that during LF refining, the tapping temperature is 1630-1690 DEG C, and the steel smelting components are controlled to include, by weight, 0.06%-0.09% of C, 0.80%-1.50% of Mn, 0.10%-0.30% of Si, not larger than 0.010% of S, not larger than 0.025% of P, 0.035%-0.060% of Ti, not l</description><language>chi ; eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170111&amp;DB=EPODOC&amp;CC=CN&amp;NR=106319352A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170111&amp;DB=EPODOC&amp;CC=CN&amp;NR=106319352A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GUAN LIUHUI</creatorcontrib><creatorcontrib>LI YONG</creatorcontrib><creatorcontrib>WEI XIAN</creatorcontrib><creatorcontrib>GUO SHIBAO</creatorcontrib><creatorcontrib>CHENG GUANJIANG</creatorcontrib><creatorcontrib>ZHOU MAOQI</creatorcontrib><creatorcontrib>WEI YUZHI</creatorcontrib><creatorcontrib>PEI FENGJUAN</creatorcontrib><creatorcontrib>ZHANG LINGZHI</creatorcontrib><creatorcontrib>XU DANGWEI</creatorcontrib><creatorcontrib>BAI JINHAN</creatorcontrib><creatorcontrib>WANG CHAOHAI</creatorcontrib><creatorcontrib>LI JINGYU</creatorcontrib><creatorcontrib>PAN SONGJUN</creatorcontrib><creatorcontrib>WANG XIANGSONG</creatorcontrib><creatorcontrib>LIU HAIQIANG</creatorcontrib><creatorcontrib>RAO JING</creatorcontrib><creatorcontrib>KONG DENAN</creatorcontrib><creatorcontrib>WANG XINJIANG</creatorcontrib><creatorcontrib>MAO JINHUA</creatorcontrib><creatorcontrib>SHANG CUNLIANG</creatorcontrib><creatorcontrib>CHEN DONGZHI</creatorcontrib><title>Titanium microalloy strengthened pipeline steel hot-rolled coiled plate and production method thereof</title><description>The invention relates to the technical field of steel materials, in particular to a titanium microalloy strengthened pipeline steel hot-rolled coiled plate and a production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate comprises the working procedures of pretreatment of molten iron, top-bottom combined blowing converter processing, LF refining, double-strand slab continuous casting, steel rolling carried out through a hot continuous rolling mill, laminar cooling and coiling. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate is characterized in that during LF refining, the tapping temperature is 1630-1690 DEG C, and the steel smelting components are controlled to include, by weight, 0.06%-0.09% of C, 0.80%-1.50% of Mn, 0.10%-0.30% of Si, not larger than 0.010% of S, not larger than 0.025% of P, 0.035%-0.060% of Ti, not l</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjbEKwkAQRNNYiPoP6wcEjEHBUoJiZZU-HJeJWdjcHpdN4d97gh9g9YaZYWZdoGVzgZeJJvZJnYi-abaE8LIRAT1FjhAOyC4gNKqVSUVy4pW_iOIM5EJWSfvFG2ugCTZqT3kjQYdtsRqczNj9uCn291vbPEpE7TBH5_OVdc2zOpzr6lKfjtf6n84HtLdAFA</recordid><startdate>20170111</startdate><enddate>20170111</enddate><creator>GUAN LIUHUI</creator><creator>LI YONG</creator><creator>WEI XIAN</creator><creator>GUO SHIBAO</creator><creator>CHENG GUANJIANG</creator><creator>ZHOU MAOQI</creator><creator>WEI YUZHI</creator><creator>PEI FENGJUAN</creator><creator>ZHANG LINGZHI</creator><creator>XU DANGWEI</creator><creator>BAI JINHAN</creator><creator>WANG CHAOHAI</creator><creator>LI JINGYU</creator><creator>PAN SONGJUN</creator><creator>WANG XIANGSONG</creator><creator>LIU HAIQIANG</creator><creator>RAO JING</creator><creator>KONG DENAN</creator><creator>WANG XINJIANG</creator><creator>MAO JINHUA</creator><creator>SHANG CUNLIANG</creator><creator>CHEN DONGZHI</creator><scope>EVB</scope></search><sort><creationdate>20170111</creationdate><title>Titanium microalloy strengthened pipeline steel hot-rolled coiled plate and production method thereof</title><author>GUAN LIUHUI ; LI YONG ; WEI XIAN ; GUO SHIBAO ; CHENG GUANJIANG ; ZHOU MAOQI ; WEI YUZHI ; PEI FENGJUAN ; ZHANG LINGZHI ; XU DANGWEI ; BAI JINHAN ; WANG CHAOHAI ; LI JINGYU ; PAN SONGJUN ; WANG XIANGSONG ; LIU HAIQIANG ; RAO JING ; KONG DENAN ; WANG XINJIANG ; MAO JINHUA ; SHANG CUNLIANG ; CHEN DONGZHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN106319352A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2017</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>GUAN LIUHUI</creatorcontrib><creatorcontrib>LI YONG</creatorcontrib><creatorcontrib>WEI XIAN</creatorcontrib><creatorcontrib>GUO SHIBAO</creatorcontrib><creatorcontrib>CHENG GUANJIANG</creatorcontrib><creatorcontrib>ZHOU MAOQI</creatorcontrib><creatorcontrib>WEI YUZHI</creatorcontrib><creatorcontrib>PEI FENGJUAN</creatorcontrib><creatorcontrib>ZHANG LINGZHI</creatorcontrib><creatorcontrib>XU DANGWEI</creatorcontrib><creatorcontrib>BAI JINHAN</creatorcontrib><creatorcontrib>WANG CHAOHAI</creatorcontrib><creatorcontrib>LI JINGYU</creatorcontrib><creatorcontrib>PAN SONGJUN</creatorcontrib><creatorcontrib>WANG XIANGSONG</creatorcontrib><creatorcontrib>LIU HAIQIANG</creatorcontrib><creatorcontrib>RAO JING</creatorcontrib><creatorcontrib>KONG DENAN</creatorcontrib><creatorcontrib>WANG XINJIANG</creatorcontrib><creatorcontrib>MAO JINHUA</creatorcontrib><creatorcontrib>SHANG CUNLIANG</creatorcontrib><creatorcontrib>CHEN DONGZHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GUAN LIUHUI</au><au>LI YONG</au><au>WEI XIAN</au><au>GUO SHIBAO</au><au>CHENG GUANJIANG</au><au>ZHOU MAOQI</au><au>WEI YUZHI</au><au>PEI FENGJUAN</au><au>ZHANG LINGZHI</au><au>XU DANGWEI</au><au>BAI JINHAN</au><au>WANG CHAOHAI</au><au>LI JINGYU</au><au>PAN SONGJUN</au><au>WANG XIANGSONG</au><au>LIU HAIQIANG</au><au>RAO JING</au><au>KONG DENAN</au><au>WANG XINJIANG</au><au>MAO JINHUA</au><au>SHANG CUNLIANG</au><au>CHEN DONGZHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Titanium microalloy strengthened pipeline steel hot-rolled coiled plate and production method thereof</title><date>2017-01-11</date><risdate>2017</risdate><abstract>The invention relates to the technical field of steel materials, in particular to a titanium microalloy strengthened pipeline steel hot-rolled coiled plate and a production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate comprises the working procedures of pretreatment of molten iron, top-bottom combined blowing converter processing, LF refining, double-strand slab continuous casting, steel rolling carried out through a hot continuous rolling mill, laminar cooling and coiling. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate is characterized in that during LF refining, the tapping temperature is 1630-1690 DEG C, and the steel smelting components are controlled to include, by weight, 0.06%-0.09% of C, 0.80%-1.50% of Mn, 0.10%-0.30% of Si, not larger than 0.010% of S, not larger than 0.025% of P, 0.035%-0.060% of Ti, not l</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN106319352A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Titanium microalloy strengthened pipeline steel hot-rolled coiled plate and production method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-14T15%3A38%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GUAN%20LIUHUI&rft.date=2017-01-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN106319352A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true