Titanium microalloy strengthened pipeline steel hot-rolled coiled plate and production method thereof

The invention relates to the technical field of steel materials, in particular to a titanium microalloy strengthened pipeline steel hot-rolled coiled plate and a production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate. The production method of the titanium mi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GUAN LIUHUI, LI YONG, WEI XIAN, GUO SHIBAO, CHENG GUANJIANG, ZHOU MAOQI, WEI YUZHI, PEI FENGJUAN, ZHANG LINGZHI, XU DANGWEI, BAI JINHAN, WANG CHAOHAI, LI JINGYU, PAN SONGJUN, WANG XIANGSONG, LIU HAIQIANG, RAO JING, KONG DENAN, WANG XINJIANG, MAO JINHUA, SHANG CUNLIANG, CHEN DONGZHI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to the technical field of steel materials, in particular to a titanium microalloy strengthened pipeline steel hot-rolled coiled plate and a production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate comprises the working procedures of pretreatment of molten iron, top-bottom combined blowing converter processing, LF refining, double-strand slab continuous casting, steel rolling carried out through a hot continuous rolling mill, laminar cooling and coiling. The production method of the titanium microalloy strengthened pipeline steel hot-rolled coiled plate is characterized in that during LF refining, the tapping temperature is 1630-1690 DEG C, and the steel smelting components are controlled to include, by weight, 0.06%-0.09% of C, 0.80%-1.50% of Mn, 0.10%-0.30% of Si, not larger than 0.010% of S, not larger than 0.025% of P, 0.035%-0.060% of Ti, not l