Method for increasing manganese leaching rate of rhodochrosite

The invention discloses a method for increasing the manganese leaching rate of rhodochrosite. The method comprises the steps that (1) concentrated sulfuric acid and water are added into rhodochrosite, the mass ratio of concentrated sulfuric acid to rhodochrosite is 1.1-1.2 times the theoretical valu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LYU KANGLE, LI JIA, MEI JINGKUN, YE HENGPENG, DU DONGYUN, LI JINLIN, CHEN MENGQI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LYU KANGLE
LI JIA
MEI JINGKUN
YE HENGPENG
DU DONGYUN
LI JINLIN
CHEN MENGQI
description The invention discloses a method for increasing the manganese leaching rate of rhodochrosite. The method comprises the steps that (1) concentrated sulfuric acid and water are added into rhodochrosite, the mass ratio of concentrated sulfuric acid to rhodochrosite is 1.1-1.2 times the theoretical value, the mass ratio of water to rhodochrosite is (6-7):1, a mixture is heated to 55-60 DEG C while being stirred, and continues to be stirred and reacted for 30-60 min, and a solid-liquid mixture is obtained; and (2) an additive, namely hexadecyl trimethyl ammonium bromide is added into the solid-liquid mixture obtained in the step (1), the mass of hexadecyl trimethyl ammonium bromide is 0.01%-0.02% of the mass of rhodochrosite, the solid-liquid mixture continues to be stirred and reacted for 3-3.5 hours at the temperature of 55-60 DEG C, and then the solid-liquid mixture is filtered to obtain filtrate, so that manganese leachate is obtained. The method is simple, operation is convenient, the cost is low, the mangane
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN106191473A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN106191473A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN106191473A3</originalsourceid><addsrcrecordid>eNrjZLDzTS3JyE9RSMsvUsjMSy5KTSzOzEtXyE3MS0_MSy1OVchJTUzOAAkVJZakKuSnKRQBlecnZxTlF2eWpPIwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0MDM0NLQxNzY0djYtQAAGZmMLg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for increasing manganese leaching rate of rhodochrosite</title><source>esp@cenet</source><creator>LYU KANGLE ; LI JIA ; MEI JINGKUN ; YE HENGPENG ; DU DONGYUN ; LI JINLIN ; CHEN MENGQI</creator><creatorcontrib>LYU KANGLE ; LI JIA ; MEI JINGKUN ; YE HENGPENG ; DU DONGYUN ; LI JINLIN ; CHEN MENGQI</creatorcontrib><description>The invention discloses a method for increasing the manganese leaching rate of rhodochrosite. The method comprises the steps that (1) concentrated sulfuric acid and water are added into rhodochrosite, the mass ratio of concentrated sulfuric acid to rhodochrosite is 1.1-1.2 times the theoretical value, the mass ratio of water to rhodochrosite is (6-7):1, a mixture is heated to 55-60 DEG C while being stirred, and continues to be stirred and reacted for 30-60 min, and a solid-liquid mixture is obtained; and (2) an additive, namely hexadecyl trimethyl ammonium bromide is added into the solid-liquid mixture obtained in the step (1), the mass of hexadecyl trimethyl ammonium bromide is 0.01%-0.02% of the mass of rhodochrosite, the solid-liquid mixture continues to be stirred and reacted for 3-3.5 hours at the temperature of 55-60 DEG C, and then the solid-liquid mixture is filtered to obtain filtrate, so that manganese leachate is obtained. The method is simple, operation is convenient, the cost is low, the mangane</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20161207&amp;DB=EPODOC&amp;CC=CN&amp;NR=106191473A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20161207&amp;DB=EPODOC&amp;CC=CN&amp;NR=106191473A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LYU KANGLE</creatorcontrib><creatorcontrib>LI JIA</creatorcontrib><creatorcontrib>MEI JINGKUN</creatorcontrib><creatorcontrib>YE HENGPENG</creatorcontrib><creatorcontrib>DU DONGYUN</creatorcontrib><creatorcontrib>LI JINLIN</creatorcontrib><creatorcontrib>CHEN MENGQI</creatorcontrib><title>Method for increasing manganese leaching rate of rhodochrosite</title><description>The invention discloses a method for increasing the manganese leaching rate of rhodochrosite. The method comprises the steps that (1) concentrated sulfuric acid and water are added into rhodochrosite, the mass ratio of concentrated sulfuric acid to rhodochrosite is 1.1-1.2 times the theoretical value, the mass ratio of water to rhodochrosite is (6-7):1, a mixture is heated to 55-60 DEG C while being stirred, and continues to be stirred and reacted for 30-60 min, and a solid-liquid mixture is obtained; and (2) an additive, namely hexadecyl trimethyl ammonium bromide is added into the solid-liquid mixture obtained in the step (1), the mass of hexadecyl trimethyl ammonium bromide is 0.01%-0.02% of the mass of rhodochrosite, the solid-liquid mixture continues to be stirred and reacted for 3-3.5 hours at the temperature of 55-60 DEG C, and then the solid-liquid mixture is filtered to obtain filtrate, so that manganese leachate is obtained. The method is simple, operation is convenient, the cost is low, the mangane</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDzTS3JyE9RSMsvUsjMSy5KTSzOzEtXyE3MS0_MSy1OVchJTUzOAAkVJZakKuSnKRQBlecnZxTlF2eWpPIwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0MDM0NLQxNzY0djYtQAAGZmMLg</recordid><startdate>20161207</startdate><enddate>20161207</enddate><creator>LYU KANGLE</creator><creator>LI JIA</creator><creator>MEI JINGKUN</creator><creator>YE HENGPENG</creator><creator>DU DONGYUN</creator><creator>LI JINLIN</creator><creator>CHEN MENGQI</creator><scope>EVB</scope></search><sort><creationdate>20161207</creationdate><title>Method for increasing manganese leaching rate of rhodochrosite</title><author>LYU KANGLE ; LI JIA ; MEI JINGKUN ; YE HENGPENG ; DU DONGYUN ; LI JINLIN ; CHEN MENGQI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN106191473A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2016</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>LYU KANGLE</creatorcontrib><creatorcontrib>LI JIA</creatorcontrib><creatorcontrib>MEI JINGKUN</creatorcontrib><creatorcontrib>YE HENGPENG</creatorcontrib><creatorcontrib>DU DONGYUN</creatorcontrib><creatorcontrib>LI JINLIN</creatorcontrib><creatorcontrib>CHEN MENGQI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LYU KANGLE</au><au>LI JIA</au><au>MEI JINGKUN</au><au>YE HENGPENG</au><au>DU DONGYUN</au><au>LI JINLIN</au><au>CHEN MENGQI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for increasing manganese leaching rate of rhodochrosite</title><date>2016-12-07</date><risdate>2016</risdate><abstract>The invention discloses a method for increasing the manganese leaching rate of rhodochrosite. The method comprises the steps that (1) concentrated sulfuric acid and water are added into rhodochrosite, the mass ratio of concentrated sulfuric acid to rhodochrosite is 1.1-1.2 times the theoretical value, the mass ratio of water to rhodochrosite is (6-7):1, a mixture is heated to 55-60 DEG C while being stirred, and continues to be stirred and reacted for 30-60 min, and a solid-liquid mixture is obtained; and (2) an additive, namely hexadecyl trimethyl ammonium bromide is added into the solid-liquid mixture obtained in the step (1), the mass of hexadecyl trimethyl ammonium bromide is 0.01%-0.02% of the mass of rhodochrosite, the solid-liquid mixture continues to be stirred and reacted for 3-3.5 hours at the temperature of 55-60 DEG C, and then the solid-liquid mixture is filtered to obtain filtrate, so that manganese leachate is obtained. The method is simple, operation is convenient, the cost is low, the mangane</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN106191473A
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Method for increasing manganese leaching rate of rhodochrosite
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-18T01%3A12%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LYU%20KANGLE&rft.date=2016-12-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN106191473A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true