Method for increasing manganese leaching rate of rhodochrosite

The invention discloses a method for increasing the manganese leaching rate of rhodochrosite. The method comprises the steps that (1) concentrated sulfuric acid and water are added into rhodochrosite, the mass ratio of concentrated sulfuric acid to rhodochrosite is 1.1-1.2 times the theoretical valu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LYU KANGLE, LI JIA, MEI JINGKUN, YE HENGPENG, DU DONGYUN, LI JINLIN, CHEN MENGQI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses a method for increasing the manganese leaching rate of rhodochrosite. The method comprises the steps that (1) concentrated sulfuric acid and water are added into rhodochrosite, the mass ratio of concentrated sulfuric acid to rhodochrosite is 1.1-1.2 times the theoretical value, the mass ratio of water to rhodochrosite is (6-7):1, a mixture is heated to 55-60 DEG C while being stirred, and continues to be stirred and reacted for 30-60 min, and a solid-liquid mixture is obtained; and (2) an additive, namely hexadecyl trimethyl ammonium bromide is added into the solid-liquid mixture obtained in the step (1), the mass of hexadecyl trimethyl ammonium bromide is 0.01%-0.02% of the mass of rhodochrosite, the solid-liquid mixture continues to be stirred and reacted for 3-3.5 hours at the temperature of 55-60 DEG C, and then the solid-liquid mixture is filtered to obtain filtrate, so that manganese leachate is obtained. The method is simple, operation is convenient, the cost is low, the mangane