Steel pipe for fuel injection line, and fuel injection line employing same
Provided is a steel pipe for a fuel injection line, having a chemical composition, expressed in weight percent, of C: 0.12-0.27%, Si: 0.05-0.40%, Mn: 0.3-2.0%, Al: 0.005-0.060%, N: 0.0020-0.0080%, Ti: 0.005-0.015%, Nb: 0.015-0.045%, Cr: 0-1.0%, Mo: 0-1.0%, Cu: 0-0.5%, Ni: 0-0.5%, V: 0-0.15%, and B:...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Provided is a steel pipe for a fuel injection line, having a chemical composition, expressed in weight percent, of C: 0.12-0.27%, Si: 0.05-0.40%, Mn: 0.3-2.0%, Al: 0.005-0.060%, N: 0.0020-0.0080%, Ti: 0.005-0.015%, Nb: 0.015-0.045%, Cr: 0-1.0%, Mo: 0-1.0%, Cu: 0-0.5%, Ni: 0-0.5%, V: 0-0.15%, and B: 0-0.005%, with the remainder being Fe and impurities. The content of Ca, P, S, and O among the impurities is Ca: 0.001% or less, P: 0.02% or less, S: 0.01% or less, and O: 0.0040% or less. The pipe has a metallographic structure comprising a tempered martensite structure or mixed structure of tempered martensite and tempered bainite, and has a prior austenite grain size number of 10.0 or above, and tensile strength TS of 800 MPa or above, as well as a critical internal pressure of at least [0.3*TS*alpha] (where alpha=[(D/d)2-1]/[0.776*(D/d)2], D: steel pipe outside diameter (mm), and d: steel pipe inside diameter (mm)).
种燃料喷射管用钢管,其化学组成以质量%计为C:0.12~0.27%、Si:0.05~0.40%、Mn:0.3~2.0%、Al:0.005~0.060%、N:0.0020~0.0080%、Ti: |
---|