Nano textile size and preparation method thereof
The invention discloses a nano textile size and a preparation method thereof. The nano textile size is prepared from components in parts by weight as follows: 80-85 parts of natural fibers, 18-25 parts of allyl phenyl isopentene ether, 15-20 parts of polyacrylamide, 12-18 parts of methacrylic acid,...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention discloses a nano textile size and a preparation method thereof. The nano textile size is prepared from components in parts by weight as follows: 80-85 parts of natural fibers, 18-25 parts of allyl phenyl isopentene ether, 15-20 parts of polyacrylamide, 12-18 parts of methacrylic acid, 8-11 parts of butyl acrylate, 5-8 parts of starch phosphate monoester, 2-4 parts of a hydroxide of (beta-hydroxyethyl) trimethyl ammonium, 2-3 parts of dimethyl 2,2-azobis(2-methylpropionate), 1-2 parts of nano zinc oxide, 1-2 parts of hydrolyzed vegetable protein, 1-2 parts of N-dodecyl mercaptan and 0.5-1 part of ammonium persulfate. The invention further provides the preparation method of the nano textile size.
本发明公开了种纳米纺织浆料及其制备方法,上述纳米纺织浆料,由包含以下重量份的组分制成:天然纤维80?85份、丙烯基苯基异戊烯醚18?25份、聚丙烯酰胺15?20份、甲基丙烯酸12?18份、丙烯酸丁酯8?11份、淀粉磷酸单酯5?8份、(β?羟乙基)三甲基氨的氢氧化物2?4份、偶氮二异丁酸二甲酯2?3份、纳米氧化锌 1?2份、水解植物蛋白1?2份、正十二硫醇1?2份和过硫酸铵0.5?1份。本发明还提供了种纳米纺织浆料的制备方法。 |
---|