Preparation method of rubber asphalt concrete

The invention discloses a preparation method of rubber asphalt concrete. The preparation method comprises the following steps of: (I) sufficiently stirring and uniformly mixing portland cement, mineral powder fly ash, stainless steel powder and green mud at 180-190 DEG C; adding rubber asphalt; and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HOU QUANHE, XIAO FENGTAO, LIU YUFENG, LIU YUANWEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HOU QUANHE
XIAO FENGTAO
LIU YUFENG
LIU YUANWEI
description The invention discloses a preparation method of rubber asphalt concrete. The preparation method comprises the following steps of: (I) sufficiently stirring and uniformly mixing portland cement, mineral powder fly ash, stainless steel powder and green mud at 180-190 DEG C; adding rubber asphalt; and stirring at 180-190 DEG C to obtain a mixture; (II) mixing limestone and blast furnace slag; calcining at 500-700 DEG C for 20-30 minutes; cooling; adding limestone and blast furnace slag into the mixture, and stirring at 180-190 DEG C for 4-8 minutes; adding water and high-calcium wastewater; and continuously stirring at 180-190 DEG C for 2-4 minutes to obtain a mixture; and (III) performing layered pouring of the mixture, vibrating and curing at 15-25 DEG C for 5-10day to obtain the rubber asphalt concrete. By adopting the preparation method disclosed by the invention, the compressive strength and crack resistance of the rubber asphalt concrete can be obviously enhanced. 本发明公开了种橡胶沥青混凝土的制备方法,包括以下步骤:步骤、将硅酸盐水泥、矿粉粉煤灰
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105801049A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105801049A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105801049A3</originalsourceid><addsrcrecordid>eNrjZNANKEotSCxKLMnMz1PITS3JyE9RyE9TKCpNSkotUkgsLshIzClRSM7PSy5KLUnlYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBqYWBoYGJpaOxsSoAQDYeypJ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of rubber asphalt concrete</title><source>esp@cenet</source><creator>HOU QUANHE ; XIAO FENGTAO ; LIU YUFENG ; LIU YUANWEI</creator><creatorcontrib>HOU QUANHE ; XIAO FENGTAO ; LIU YUFENG ; LIU YUANWEI</creatorcontrib><description>The invention discloses a preparation method of rubber asphalt concrete. The preparation method comprises the following steps of: (I) sufficiently stirring and uniformly mixing portland cement, mineral powder fly ash, stainless steel powder and green mud at 180-190 DEG C; adding rubber asphalt; and stirring at 180-190 DEG C to obtain a mixture; (II) mixing limestone and blast furnace slag; calcining at 500-700 DEG C for 20-30 minutes; cooling; adding limestone and blast furnace slag into the mixture, and stirring at 180-190 DEG C for 4-8 minutes; adding water and high-calcium wastewater; and continuously stirring at 180-190 DEG C for 2-4 minutes to obtain a mixture; and (III) performing layered pouring of the mixture, vibrating and curing at 15-25 DEG C for 5-10day to obtain the rubber asphalt concrete. By adopting the preparation method disclosed by the invention, the compressive strength and crack resistance of the rubber asphalt concrete can be obviously enhanced. 本发明公开了种橡胶沥青混凝土的制备方法,包括以下步骤:步骤、将硅酸盐水泥、矿粉粉煤灰</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATERTREATMENT OR WASTE MANAGEMENT ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC ; GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS ; TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE ; TREATMENT OF NATURAL STONE</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160727&amp;DB=EPODOC&amp;CC=CN&amp;NR=105801049A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160727&amp;DB=EPODOC&amp;CC=CN&amp;NR=105801049A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HOU QUANHE</creatorcontrib><creatorcontrib>XIAO FENGTAO</creatorcontrib><creatorcontrib>LIU YUFENG</creatorcontrib><creatorcontrib>LIU YUANWEI</creatorcontrib><title>Preparation method of rubber asphalt concrete</title><description>The invention discloses a preparation method of rubber asphalt concrete. The preparation method comprises the following steps of: (I) sufficiently stirring and uniformly mixing portland cement, mineral powder fly ash, stainless steel powder and green mud at 180-190 DEG C; adding rubber asphalt; and stirring at 180-190 DEG C to obtain a mixture; (II) mixing limestone and blast furnace slag; calcining at 500-700 DEG C for 20-30 minutes; cooling; adding limestone and blast furnace slag into the mixture, and stirring at 180-190 DEG C for 4-8 minutes; adding water and high-calcium wastewater; and continuously stirring at 180-190 DEG C for 2-4 minutes to obtain a mixture; and (III) performing layered pouring of the mixture, vibrating and curing at 15-25 DEG C for 5-10day to obtain the rubber asphalt concrete. By adopting the preparation method disclosed by the invention, the compressive strength and crack resistance of the rubber asphalt concrete can be obviously enhanced. 本发明公开了种橡胶沥青混凝土的制备方法,包括以下步骤:步骤、将硅酸盐水泥、矿粉粉煤灰</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATERTREATMENT OR WASTE MANAGEMENT</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</subject><subject>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</subject><subject>TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNANKEotSCxKLMnMz1PITS3JyE9RyE9TKCpNSkotUkgsLshIzClRSM7PSy5KLUnlYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBqYWBoYGJpaOxsSoAQDYeypJ</recordid><startdate>20160727</startdate><enddate>20160727</enddate><creator>HOU QUANHE</creator><creator>XIAO FENGTAO</creator><creator>LIU YUFENG</creator><creator>LIU YUANWEI</creator><scope>EVB</scope></search><sort><creationdate>20160727</creationdate><title>Preparation method of rubber asphalt concrete</title><author>HOU QUANHE ; XIAO FENGTAO ; LIU YUFENG ; LIU YUANWEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105801049A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2016</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATERTREATMENT OR WASTE MANAGEMENT</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</topic><topic>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</topic><topic>TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>HOU QUANHE</creatorcontrib><creatorcontrib>XIAO FENGTAO</creatorcontrib><creatorcontrib>LIU YUFENG</creatorcontrib><creatorcontrib>LIU YUANWEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HOU QUANHE</au><au>XIAO FENGTAO</au><au>LIU YUFENG</au><au>LIU YUANWEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of rubber asphalt concrete</title><date>2016-07-27</date><risdate>2016</risdate><abstract>The invention discloses a preparation method of rubber asphalt concrete. The preparation method comprises the following steps of: (I) sufficiently stirring and uniformly mixing portland cement, mineral powder fly ash, stainless steel powder and green mud at 180-190 DEG C; adding rubber asphalt; and stirring at 180-190 DEG C to obtain a mixture; (II) mixing limestone and blast furnace slag; calcining at 500-700 DEG C for 20-30 minutes; cooling; adding limestone and blast furnace slag into the mixture, and stirring at 180-190 DEG C for 4-8 minutes; adding water and high-calcium wastewater; and continuously stirring at 180-190 DEG C for 2-4 minutes to obtain a mixture; and (III) performing layered pouring of the mixture, vibrating and curing at 15-25 DEG C for 5-10day to obtain the rubber asphalt concrete. By adopting the preparation method disclosed by the invention, the compressive strength and crack resistance of the rubber asphalt concrete can be obviously enhanced. 本发明公开了种橡胶沥青混凝土的制备方法,包括以下步骤:步骤、将硅酸盐水泥、矿粉粉煤灰</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN105801049A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATERTREATMENT OR WASTE MANAGEMENT
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE
TREATMENT OF NATURAL STONE
title Preparation method of rubber asphalt concrete
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T02%3A19%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HOU%20QUANHE&rft.date=2016-07-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105801049A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true