Preparation method of rubber asphalt concrete

The invention discloses a preparation method of rubber asphalt concrete. The preparation method comprises the following steps of: (I) sufficiently stirring and uniformly mixing portland cement, mineral powder fly ash, stainless steel powder and green mud at 180-190 DEG C; adding rubber asphalt; and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HOU QUANHE, XIAO FENGTAO, LIU YUFENG, LIU YUANWEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses a preparation method of rubber asphalt concrete. The preparation method comprises the following steps of: (I) sufficiently stirring and uniformly mixing portland cement, mineral powder fly ash, stainless steel powder and green mud at 180-190 DEG C; adding rubber asphalt; and stirring at 180-190 DEG C to obtain a mixture; (II) mixing limestone and blast furnace slag; calcining at 500-700 DEG C for 20-30 minutes; cooling; adding limestone and blast furnace slag into the mixture, and stirring at 180-190 DEG C for 4-8 minutes; adding water and high-calcium wastewater; and continuously stirring at 180-190 DEG C for 2-4 minutes to obtain a mixture; and (III) performing layered pouring of the mixture, vibrating and curing at 15-25 DEG C for 5-10day to obtain the rubber asphalt concrete. By adopting the preparation method disclosed by the invention, the compressive strength and crack resistance of the rubber asphalt concrete can be obviously enhanced. 本发明公开了种橡胶沥青混凝土的制备方法,包括以下步骤:步骤、将硅酸盐水泥、矿粉粉煤灰