Degradable golf tee and preparing method thereof
The invention relates to a degradable golf tee. The golf tee is prepared from, by weight, 80-120 parts of coal ash, 10-30 parts of clay, 2-5 parts of sodium citrate, 1-5 parts of water reducer, 8-15 parts of air entraining agent, 1-5 parts of accelerator and 120-200 parts of water. By preparing the...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a degradable golf tee. The golf tee is prepared from, by weight, 80-120 parts of coal ash, 10-30 parts of clay, 2-5 parts of sodium citrate, 1-5 parts of water reducer, 8-15 parts of air entraining agent, 1-5 parts of accelerator and 120-200 parts of water. By preparing the golf tee with the method, coal ash can be sufficiently and reasonably utilized, pollution to the atmosphere caused by coal ash is reduced, and production cost is reduced greatly; secondary pollution might be caused to the environment during recycling of plastic golf tees, however, the golf tee made from coal ash does not need to be recycled after being used and can be degraded in a meadow so as to become good meadow maintenance fertilizer. |
---|