Low-cost anaerobic adhesive and preparation method thereof

The invention relates to a low-cost anaerobic adhesive and a preparation method thereof. The anaerobic adhesive is prepared from the following components in percentage by weight: 36.0%-45.2% of an acrylic ester oligomer, 8.8%-11.1% of an acrylate monomer, 1.0%-2.0% of a stabilizer, 2.0%-3.0% of an a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GAO ZHOU, SUN YUSHENG, HUANG YI, HONG JIAN, LIU YONGGANG, YOU RENGUO, LEI MUSHENG
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GAO ZHOU
SUN YUSHENG
HUANG YI
HONG JIAN
LIU YONGGANG
YOU RENGUO
LEI MUSHENG
description The invention relates to a low-cost anaerobic adhesive and a preparation method thereof. The anaerobic adhesive is prepared from the following components in percentage by weight: 36.0%-45.2% of an acrylic ester oligomer, 8.8%-11.1% of an acrylate monomer, 1.0%-2.0% of a stabilizer, 2.0%-3.0% of an accelerant, 30.0%-40.0% of silica powder, 7.5%-10.0% of hollow glass beads, 1.0%-2.0% of an initiator and 0.1%-0.4% of a dye. The preparation method comprises the following steps: adding the acrylic ester oligomer, the acrylate monomer, the stabilizer and the accelerant to a power mixer, and stirring evenly until various components are fully dissolved; and sequentially adding the silica powder and the hollow glass beads, mixing the silica powder and the hollow glass beads evenly, adding the initiator and the dye, and stirring and mixing until the dye is fully dissolved. The low-cost anaerobic adhesive provided by the invention is relatively fast in curing speed and relatively high in curing strength, and has excellent storage stability; and the cost is reduced by over 30%.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105176422A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105176422A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105176422A3</originalsourceid><addsrcrecordid>eNrjZLDyyS_XTc4vLlFIzEtMLcpPykxWSEzJSC3OLEsFCqUoFBSlFiQWJZZk5ucp5KaWZOSnKJRkpBal5qfxMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DA1NDczMTIyNHY2LUAACASC8k</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Low-cost anaerobic adhesive and preparation method thereof</title><source>esp@cenet</source><creator>GAO ZHOU ; SUN YUSHENG ; HUANG YI ; HONG JIAN ; LIU YONGGANG ; YOU RENGUO ; LEI MUSHENG</creator><creatorcontrib>GAO ZHOU ; SUN YUSHENG ; HUANG YI ; HONG JIAN ; LIU YONGGANG ; YOU RENGUO ; LEI MUSHENG</creatorcontrib><description>The invention relates to a low-cost anaerobic adhesive and a preparation method thereof. The anaerobic adhesive is prepared from the following components in percentage by weight: 36.0%-45.2% of an acrylic ester oligomer, 8.8%-11.1% of an acrylate monomer, 1.0%-2.0% of a stabilizer, 2.0%-3.0% of an accelerant, 30.0%-40.0% of silica powder, 7.5%-10.0% of hollow glass beads, 1.0%-2.0% of an initiator and 0.1%-0.4% of a dye. The preparation method comprises the following steps: adding the acrylic ester oligomer, the acrylate monomer, the stabilizer and the accelerant to a power mixer, and stirring evenly until various components are fully dissolved; and sequentially adding the silica powder and the hollow glass beads, mixing the silica powder and the hollow glass beads evenly, adding the initiator and the dye, and stirring and mixing until the dye is fully dissolved. The low-cost anaerobic adhesive provided by the invention is relatively fast in curing speed and relatively high in curing strength, and has excellent storage stability; and the cost is reduced by over 30%.</description><language>eng</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; CHEMISTRY ; DYES ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; PAINTS ; POLISHES ; USE OF MATERIALS AS ADHESIVES</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151223&amp;DB=EPODOC&amp;CC=CN&amp;NR=105176422A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151223&amp;DB=EPODOC&amp;CC=CN&amp;NR=105176422A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GAO ZHOU</creatorcontrib><creatorcontrib>SUN YUSHENG</creatorcontrib><creatorcontrib>HUANG YI</creatorcontrib><creatorcontrib>HONG JIAN</creatorcontrib><creatorcontrib>LIU YONGGANG</creatorcontrib><creatorcontrib>YOU RENGUO</creatorcontrib><creatorcontrib>LEI MUSHENG</creatorcontrib><title>Low-cost anaerobic adhesive and preparation method thereof</title><description>The invention relates to a low-cost anaerobic adhesive and a preparation method thereof. The anaerobic adhesive is prepared from the following components in percentage by weight: 36.0%-45.2% of an acrylic ester oligomer, 8.8%-11.1% of an acrylate monomer, 1.0%-2.0% of a stabilizer, 2.0%-3.0% of an accelerant, 30.0%-40.0% of silica powder, 7.5%-10.0% of hollow glass beads, 1.0%-2.0% of an initiator and 0.1%-0.4% of a dye. The preparation method comprises the following steps: adding the acrylic ester oligomer, the acrylate monomer, the stabilizer and the accelerant to a power mixer, and stirring evenly until various components are fully dissolved; and sequentially adding the silica powder and the hollow glass beads, mixing the silica powder and the hollow glass beads evenly, adding the initiator and the dye, and stirring and mixing until the dye is fully dissolved. The low-cost anaerobic adhesive provided by the invention is relatively fast in curing speed and relatively high in curing strength, and has excellent storage stability; and the cost is reduced by over 30%.</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDyyS_XTc4vLlFIzEtMLcpPykxWSEzJSC3OLEsFCqUoFBSlFiQWJZZk5ucp5KaWZOSnKJRkpBal5qfxMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DA1NDczMTIyNHY2LUAACASC8k</recordid><startdate>20151223</startdate><enddate>20151223</enddate><creator>GAO ZHOU</creator><creator>SUN YUSHENG</creator><creator>HUANG YI</creator><creator>HONG JIAN</creator><creator>LIU YONGGANG</creator><creator>YOU RENGUO</creator><creator>LEI MUSHENG</creator><scope>EVB</scope></search><sort><creationdate>20151223</creationdate><title>Low-cost anaerobic adhesive and preparation method thereof</title><author>GAO ZHOU ; SUN YUSHENG ; HUANG YI ; HONG JIAN ; LIU YONGGANG ; YOU RENGUO ; LEI MUSHENG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105176422A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>GAO ZHOU</creatorcontrib><creatorcontrib>SUN YUSHENG</creatorcontrib><creatorcontrib>HUANG YI</creatorcontrib><creatorcontrib>HONG JIAN</creatorcontrib><creatorcontrib>LIU YONGGANG</creatorcontrib><creatorcontrib>YOU RENGUO</creatorcontrib><creatorcontrib>LEI MUSHENG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GAO ZHOU</au><au>SUN YUSHENG</au><au>HUANG YI</au><au>HONG JIAN</au><au>LIU YONGGANG</au><au>YOU RENGUO</au><au>LEI MUSHENG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Low-cost anaerobic adhesive and preparation method thereof</title><date>2015-12-23</date><risdate>2015</risdate><abstract>The invention relates to a low-cost anaerobic adhesive and a preparation method thereof. The anaerobic adhesive is prepared from the following components in percentage by weight: 36.0%-45.2% of an acrylic ester oligomer, 8.8%-11.1% of an acrylate monomer, 1.0%-2.0% of a stabilizer, 2.0%-3.0% of an accelerant, 30.0%-40.0% of silica powder, 7.5%-10.0% of hollow glass beads, 1.0%-2.0% of an initiator and 0.1%-0.4% of a dye. The preparation method comprises the following steps: adding the acrylic ester oligomer, the acrylate monomer, the stabilizer and the accelerant to a power mixer, and stirring evenly until various components are fully dissolved; and sequentially adding the silica powder and the hollow glass beads, mixing the silica powder and the hollow glass beads evenly, adding the initiator and the dye, and stirring and mixing until the dye is fully dissolved. The low-cost anaerobic adhesive provided by the invention is relatively fast in curing speed and relatively high in curing strength, and has excellent storage stability; and the cost is reduced by over 30%.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN105176422A
source esp@cenet
subjects ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE
ADHESIVES
CHEMISTRY
DYES
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL
PAINTS
POLISHES
USE OF MATERIALS AS ADHESIVES
title Low-cost anaerobic adhesive and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T18%3A15%3A47IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GAO%20ZHOU&rft.date=2015-12-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105176422A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true