Laser-arc hybrid welding method of medium-thickness board corner joint
The invention provides a laser-arc hybrid welding method of a medium-thickness board corner joint. The laser-arc hybrid welding method comprises the following steps that 1, the corner joint and welded test boards are adjusted to enable weld joints to be ship-shaped; 2, a laser instrument is adjusted...
Gespeichert in:
Hauptverfasser: | , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | YUN ZHONGHUANG LIANG LIANJIE GE HUAIPU SUI XIANTING HUO QIAOYING LI DONGFENG DAI ZHONGCHEN XUE HAIFENG GUO YI |
description | The invention provides a laser-arc hybrid welding method of a medium-thickness board corner joint. The laser-arc hybrid welding method comprises the following steps that 1, the corner joint and welded test boards are adjusted to enable weld joints to be ship-shaped; 2, a laser instrument is adjusted to enable a laser beam transmitted by the laser instrument to be perpendicular to the weld joints; 3, an arc welding gun is adjusted to enable a gun head of the arc welding gun not to interfere with the test board 1 and the test board 2 on two sides, wherein the included angle formed by the straight line where the gun head is located and the laser beam is theta 3. According to the laser-arc hybrid welding method, the space positions of the gun head of the welding gun and the laser beam are technologically adjusted to enable the advancing directions of the gun head and the laser beam not to be located in the same plane. Therefore, limited fusion penetration of laser to the diagonal weld joints is ensured, the advantages of laser-arc hybrid welding can be also kept, and the laser-arc hybrid welding method can be widely applied to welding of the medium-thickness board corner joint. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105171243A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105171243A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105171243A3</originalsourceid><addsrcrecordid>eNrjZHDzSSxOLdJNLEpWyKhMKspMUShPzUnJzEtXyE0tychPUchPA7JSMktzdUsyMpOz81KLixWS8hOLUhSS84vyUosUsvIz80p4GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hgamhuaGRibGjMTFqABkaM2g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Laser-arc hybrid welding method of medium-thickness board corner joint</title><source>esp@cenet</source><creator>YUN ZHONGHUANG ; LIANG LIANJIE ; GE HUAIPU ; SUI XIANTING ; HUO QIAOYING ; LI DONGFENG ; DAI ZHONGCHEN ; XUE HAIFENG ; GUO YI</creator><creatorcontrib>YUN ZHONGHUANG ; LIANG LIANJIE ; GE HUAIPU ; SUI XIANTING ; HUO QIAOYING ; LI DONGFENG ; DAI ZHONGCHEN ; XUE HAIFENG ; GUO YI</creatorcontrib><description>The invention provides a laser-arc hybrid welding method of a medium-thickness board corner joint. The laser-arc hybrid welding method comprises the following steps that 1, the corner joint and welded test boards are adjusted to enable weld joints to be ship-shaped; 2, a laser instrument is adjusted to enable a laser beam transmitted by the laser instrument to be perpendicular to the weld joints; 3, an arc welding gun is adjusted to enable a gun head of the arc welding gun not to interfere with the test board 1 and the test board 2 on two sides, wherein the included angle formed by the straight line where the gun head is located and the laser beam is theta 3. According to the laser-arc hybrid welding method, the space positions of the gun head of the welding gun and the laser beam are technologically adjusted to enable the advancing directions of the gun head and the laser beam not to be located in the same plane. Therefore, limited fusion penetration of laser to the diagonal weld joints is ensured, the advantages of laser-arc hybrid welding can be also kept, and the laser-arc hybrid welding method can be widely applied to welding of the medium-thickness board corner joint.</description><language>eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20151223&DB=EPODOC&CC=CN&NR=105171243A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20151223&DB=EPODOC&CC=CN&NR=105171243A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YUN ZHONGHUANG</creatorcontrib><creatorcontrib>LIANG LIANJIE</creatorcontrib><creatorcontrib>GE HUAIPU</creatorcontrib><creatorcontrib>SUI XIANTING</creatorcontrib><creatorcontrib>HUO QIAOYING</creatorcontrib><creatorcontrib>LI DONGFENG</creatorcontrib><creatorcontrib>DAI ZHONGCHEN</creatorcontrib><creatorcontrib>XUE HAIFENG</creatorcontrib><creatorcontrib>GUO YI</creatorcontrib><title>Laser-arc hybrid welding method of medium-thickness board corner joint</title><description>The invention provides a laser-arc hybrid welding method of a medium-thickness board corner joint. The laser-arc hybrid welding method comprises the following steps that 1, the corner joint and welded test boards are adjusted to enable weld joints to be ship-shaped; 2, a laser instrument is adjusted to enable a laser beam transmitted by the laser instrument to be perpendicular to the weld joints; 3, an arc welding gun is adjusted to enable a gun head of the arc welding gun not to interfere with the test board 1 and the test board 2 on two sides, wherein the included angle formed by the straight line where the gun head is located and the laser beam is theta 3. According to the laser-arc hybrid welding method, the space positions of the gun head of the welding gun and the laser beam are technologically adjusted to enable the advancing directions of the gun head and the laser beam not to be located in the same plane. Therefore, limited fusion penetration of laser to the diagonal weld joints is ensured, the advantages of laser-arc hybrid welding can be also kept, and the laser-arc hybrid welding method can be widely applied to welding of the medium-thickness board corner joint.</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDzSSxOLdJNLEpWyKhMKspMUShPzUnJzEtXyE0tychPUchPA7JSMktzdUsyMpOz81KLixWS8hOLUhSS84vyUosUsvIz80p4GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hgamhuaGRibGjMTFqABkaM2g</recordid><startdate>20151223</startdate><enddate>20151223</enddate><creator>YUN ZHONGHUANG</creator><creator>LIANG LIANJIE</creator><creator>GE HUAIPU</creator><creator>SUI XIANTING</creator><creator>HUO QIAOYING</creator><creator>LI DONGFENG</creator><creator>DAI ZHONGCHEN</creator><creator>XUE HAIFENG</creator><creator>GUO YI</creator><scope>EVB</scope></search><sort><creationdate>20151223</creationdate><title>Laser-arc hybrid welding method of medium-thickness board corner joint</title><author>YUN ZHONGHUANG ; LIANG LIANJIE ; GE HUAIPU ; SUI XIANTING ; HUO QIAOYING ; LI DONGFENG ; DAI ZHONGCHEN ; XUE HAIFENG ; GUO YI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105171243A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>YUN ZHONGHUANG</creatorcontrib><creatorcontrib>LIANG LIANJIE</creatorcontrib><creatorcontrib>GE HUAIPU</creatorcontrib><creatorcontrib>SUI XIANTING</creatorcontrib><creatorcontrib>HUO QIAOYING</creatorcontrib><creatorcontrib>LI DONGFENG</creatorcontrib><creatorcontrib>DAI ZHONGCHEN</creatorcontrib><creatorcontrib>XUE HAIFENG</creatorcontrib><creatorcontrib>GUO YI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YUN ZHONGHUANG</au><au>LIANG LIANJIE</au><au>GE HUAIPU</au><au>SUI XIANTING</au><au>HUO QIAOYING</au><au>LI DONGFENG</au><au>DAI ZHONGCHEN</au><au>XUE HAIFENG</au><au>GUO YI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Laser-arc hybrid welding method of medium-thickness board corner joint</title><date>2015-12-23</date><risdate>2015</risdate><abstract>The invention provides a laser-arc hybrid welding method of a medium-thickness board corner joint. The laser-arc hybrid welding method comprises the following steps that 1, the corner joint and welded test boards are adjusted to enable weld joints to be ship-shaped; 2, a laser instrument is adjusted to enable a laser beam transmitted by the laser instrument to be perpendicular to the weld joints; 3, an arc welding gun is adjusted to enable a gun head of the arc welding gun not to interfere with the test board 1 and the test board 2 on two sides, wherein the included angle formed by the straight line where the gun head is located and the laser beam is theta 3. According to the laser-arc hybrid welding method, the space positions of the gun head of the welding gun and the laser beam are technologically adjusted to enable the advancing directions of the gun head and the laser beam not to be located in the same plane. Therefore, limited fusion penetration of laser to the diagonal weld joints is ensured, the advantages of laser-arc hybrid welding can be also kept, and the laser-arc hybrid welding method can be widely applied to welding of the medium-thickness board corner joint.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_CN105171243A |
source | esp@cenet |
subjects | CLADDING OR PLATING BY SOLDERING OR WELDING CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR PERFORMING OPERATIONS SOLDERING OR UNSOLDERING TRANSPORTING WELDING WORKING BY LASER BEAM |
title | Laser-arc hybrid welding method of medium-thickness board corner joint |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T07%3A36%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YUN%20ZHONGHUANG&rft.date=2015-12-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105171243A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |