Water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof
The invention discloses a water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof. The emulsion is characterized in that it comprises the following components by mass percentage: 30-50% of maleic anhydride modified polypropylene wax 1, 10-20% of maleic...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | KONG XIAOYIN |
description | The invention discloses a water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof. The emulsion is characterized in that it comprises the following components by mass percentage: 30-50% of maleic anhydride modified polypropylene wax 1, 10-20% of maleic anhydride modified polypropylene wax 2, 10%-35% of a solvent, 4%-9.5% of an ethylene oxide-propylene oxide block polymer 1, 3%-6.5% of an ethylene oxide-propylene oxide block polymer 2, 4%-10% of an alcohol amine compound, 0.1%-1% of p-toluenesulfonic acid, and 2-5% of an acidifier. Compared with some imported emulsion, the emulsion provided by the invention has a storage period extended by 90 days under normal temperature, and is still stable after preservation at a temperature of -40DEG C for 90 days, while demulsification can occur to the imported emulsion on the 65th day. The storage period of the emulsion can reach 120 days under a 60DEG C environment, while the storage period of the imported emulsion is 50 days. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105060736A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105060736A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105060736A3</originalsourceid><addsrcrecordid>eNqNjDsKwkAURdNYiLqH5wKESDDWEhQrSSFYhpfMHTMwP2ZeCndvAi7A6sLhnLsu3i8WJMrBTr0FObYwA7EfPyoZNYOgjDZQ1LYEN9lsgicdEmnTL92UNA8gSWBx8DKnijhGawaWxZURCUFvi5Vmm7H77abY367P5n5ADB1ynE88pGsex_JU1uW5qi_VP84Xv-pADw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof</title><source>esp@cenet</source><creator>KONG XIAOYIN</creator><creatorcontrib>KONG XIAOYIN</creatorcontrib><description>The invention discloses a water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof. The emulsion is characterized in that it comprises the following components by mass percentage: 30-50% of maleic anhydride modified polypropylene wax 1, 10-20% of maleic anhydride modified polypropylene wax 2, 10%-35% of a solvent, 4%-9.5% of an ethylene oxide-propylene oxide block polymer 1, 3%-6.5% of an ethylene oxide-propylene oxide block polymer 2, 4%-10% of an alcohol amine compound, 0.1%-1% of p-toluenesulfonic acid, and 2-5% of an acidifier. Compared with some imported emulsion, the emulsion provided by the invention has a storage period extended by 90 days under normal temperature, and is still stable after preservation at a temperature of -40DEG C for 90 days, while demulsification can occur to the imported emulsion on the 65th day. The storage period of the emulsion can reach 120 days under a 60DEG C environment, while the storage period of the imported emulsion is 50 days.</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20151118&DB=EPODOC&CC=CN&NR=105060736A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20151118&DB=EPODOC&CC=CN&NR=105060736A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KONG XIAOYIN</creatorcontrib><title>Water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof</title><description>The invention discloses a water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof. The emulsion is characterized in that it comprises the following components by mass percentage: 30-50% of maleic anhydride modified polypropylene wax 1, 10-20% of maleic anhydride modified polypropylene wax 2, 10%-35% of a solvent, 4%-9.5% of an ethylene oxide-propylene oxide block polymer 1, 3%-6.5% of an ethylene oxide-propylene oxide block polymer 2, 4%-10% of an alcohol amine compound, 0.1%-1% of p-toluenesulfonic acid, and 2-5% of an acidifier. Compared with some imported emulsion, the emulsion provided by the invention has a storage period extended by 90 days under normal temperature, and is still stable after preservation at a temperature of -40DEG C for 90 days, while demulsification can occur to the imported emulsion on the 65th day. The storage period of the emulsion can reach 120 days under a 60DEG C environment, while the storage period of the imported emulsion is 50 days.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjDsKwkAURdNYiLqH5wKESDDWEhQrSSFYhpfMHTMwP2ZeCndvAi7A6sLhnLsu3i8WJMrBTr0FObYwA7EfPyoZNYOgjDZQ1LYEN9lsgicdEmnTL92UNA8gSWBx8DKnijhGawaWxZURCUFvi5Vmm7H77abY367P5n5ADB1ynE88pGsex_JU1uW5qi_VP84Xv-pADw</recordid><startdate>20151118</startdate><enddate>20151118</enddate><creator>KONG XIAOYIN</creator><scope>EVB</scope></search><sort><creationdate>20151118</creationdate><title>Water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof</title><author>KONG XIAOYIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105060736A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>KONG XIAOYIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KONG XIAOYIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof</title><date>2015-11-18</date><risdate>2015</risdate><abstract>The invention discloses a water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof. The emulsion is characterized in that it comprises the following components by mass percentage: 30-50% of maleic anhydride modified polypropylene wax 1, 10-20% of maleic anhydride modified polypropylene wax 2, 10%-35% of a solvent, 4%-9.5% of an ethylene oxide-propylene oxide block polymer 1, 3%-6.5% of an ethylene oxide-propylene oxide block polymer 2, 4%-10% of an alcohol amine compound, 0.1%-1% of p-toluenesulfonic acid, and 2-5% of an acidifier. Compared with some imported emulsion, the emulsion provided by the invention has a storage period extended by 90 days under normal temperature, and is still stable after preservation at a temperature of -40DEG C for 90 days, while demulsification can occur to the imported emulsion on the 65th day. The storage period of the emulsion can reach 120 days under a 60DEG C environment, while the storage period of the imported emulsion is 50 days.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_CN105060736A |
source | esp@cenet |
subjects | CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS CHEMISTRY GLASS JOINING GLASS TO GLASS OR OTHER MATERIALS METALLURGY MINERAL OR SLAG WOOL SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS SURFACE TREATMENT OF GLASS |
title | Water soluble maleic anhydride modified PP emulsion for fiber surface treatment and application thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T16%3A55%3A29IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KONG%20XIAOYIN&rft.date=2015-11-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105060736A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |