Inorganic modified asphalt and preparation method thereof

The invention relates to inorganic modified asphalt and a preparation method thereof, wherein the inorganic modified asphalt is prepared by mixing the following raw materials comprising, by weight, 100 parts of basic asphalt, 5.5-15.5 parts of boracites, 3.5-10.5 parts of albite, 4-8 parts of silica...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GAO ZHIWEI, ZHU BIN, YAN XIHUA, WANG CHAOHUI, LIU JUN, LIAN XIANGPING, SUN XIAOLONG, WANG ZHIHUA, LI JIFANG, FENG WEI, ZHENG JIANFENG, ZHEN XI, DI SHENGGUAN, ZHANG GUISHENG, WANG XIAOHUA, YANG YUE, LIU RUNYOU, XU ZHENZHEN, WANG XINQI, LIANG YICHAO, HE HAI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to inorganic modified asphalt and a preparation method thereof, wherein the inorganic modified asphalt is prepared by mixing the following raw materials comprising, by weight, 100 parts of basic asphalt, 5.5-15.5 parts of boracites, 3.5-10.5 parts of albite, 4-8 parts of silica gel powder, 1-2 parts of microcrystalline cellulose, 0.5-1 part of triethanolamine and 2-4 parts of an additive being extract oil of Iran rubber oil or furfural extract oil. The inorganic modified asphalt is significant in temperature-controlling effect, is low in cost, is simple in preparation process and is convenient to construct.