Preparation method of shock-resistant and deformation-resistant modified polylactic acid material

Through mixing extrusion of 70-80% of polylactic acid with the molecular weight of 20000-200000, 10-20% of a plasticizer, 5-10% of a toughening agent, 0.5-1% of an antioxidant and 0.5% of a coupling agent, the material toughness and plasticity are greatly improved, and a shock-resistant and deformat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LU JIANXIN, JIA YUCHONG, GONG KE'NAN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Through mixing extrusion of 70-80% of polylactic acid with the molecular weight of 20000-200000, 10-20% of a plasticizer, 5-10% of a toughening agent, 0.5-1% of an antioxidant and 0.5% of a coupling agent, the material toughness and plasticity are greatly improved, and a shock-resistant and deformation-resistant modified PLA material is obtained.