Integrated nano-toughened PA6 nanocomposite material
The invention discloses an integrated nano-toughened PA6 nanocomposite material. The integrated nano-toughened PA6 nanocomposite material comprises the following raw materials in parts by mass: 70-90 parts of PA6, 10-20 parts of PE, 0.5-5 parts of maleic anhydride, 0.1-0.3 part of an antioxygen, 0.0...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention discloses an integrated nano-toughened PA6 nanocomposite material. The integrated nano-toughened PA6 nanocomposite material comprises the following raw materials in parts by mass: 70-90 parts of PA6, 10-20 parts of PE, 0.5-5 parts of maleic anhydride, 0.1-0.3 part of an antioxygen, 0.05-0.1 part of a catalyst I, 0.05-0.1 part of a catalyst II and 1-3 parts of nanoemulsion, wherein the nanoemulsion is prepared in the following steps: 1), adding 1-3 parts of nanopowder into a coupling agent solution, and uniformly mixing; 2) regulating pH to be 6.5-7.5; 3) performing ultrasonic dispersion into the uniform emulsion. Through integral formula design, the catalyst I and the catalyst II are introduced into a system; in the preparation process of the composite material, in-situ grafting can be achieved; through cooperation of a matrix and various functional auxiliary agents, the toughness of nylon is greatly improved. |
---|