Method for producing high-molecular-weight polyisobutylene

The invention relates to the production of isobutylene homopolymers having a weight-average molecular weight of 75,000 to 10,000,000 by means of the polymerization of isobutylene by (a) performing the polymerization at -80 DEG C to -190 DEG C, (b) using optionally halogenated C1 to C5 hydrocarbons a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BRYM MARKUS, DAISS ANDREAS, CORBERAN ROC ROSA, WETTLING THOMAS, HIRSCH STEFAN, WEIS MARKUS, VOLLAND MARCO CHRISTIAN, MUEHLBACH KLAUS, HASCHICK ROBERT
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to the production of isobutylene homopolymers having a weight-average molecular weight of 75,000 to 10,000,000 by means of the polymerization of isobutylene by (a) performing the polymerization at -80 DEG C to -190 DEG C, (b) using optionally halogenated C1 to C5 hydrocarbons as an inert solvent, (c) using a Lewis acid complex as a polymerization catalyst, and (d) performing the polymerization in the presence of at least one reaction accelerator in the form of an ethylenically saturated hydrocarbon compound, which contains an oxygen atom and no proton that can be emitted, and performing the polymerization in the presence of at least one chain length regulator, which contains a tertiary olefinic carbon atom.