Method and device for grinding metal annular member
Provided is a grinding method capable of preventing variations in the outer diameter of a workpiece (1) at the completion of grinding regardless of variations in the amount of elastic deformation of the workpiece (1) based on changes in a whetstone (4) sharpening ability and the like. The outer diam...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Provided is a grinding method capable of preventing variations in the outer diameter of a workpiece (1) at the completion of grinding regardless of variations in the amount of elastic deformation of the workpiece (1) based on changes in a whetstone (4) sharpening ability and the like. The outer diameter (D) of the workpiece (1) during grinding is measured, in process, by a gauge head (5). A plurality of mutually different target values Di are specified in relation to the outer diameter (D) of the workpiece (1), and a first threshold pertaining to the rate of change of the outer diameter (D) of the workpiece (1) is specified for each of the target values Di. A spark-out starts when the absolute value of the rate of change v, when the outer diameter (D) of the workpiece (1) reaches a target value Di, exceeds the first threshold corresponding to the target value Di. |
---|