The invention discloses a manufacturing method for pattern adding and bending glass. The manufacturing method comprise the following steps: (1) adding patterns: glass paint with high temperature is taken to add patterns on the glass, wherein the glass paint is prepared from the following materials:...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: FENG JIYAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses a manufacturing method for pattern adding and bending glass. The manufacturing method comprise the following steps: (1) adding patterns: glass paint with high temperature is taken to add patterns on the glass, wherein the glass paint is prepared from the following materials: 11-12 parts of hydroxyethyl cellulose, 4-6 parts of talcum powder, 3-5 parts of alkali bismuth chloride, 5-6 parts of dissolving resin, 3-4 parts of butyl alcohol, 5-6 parts of butyl stearate, 2-4 parts of gloss oil, and 30-40 parts of water; the temperature of the glass paint is 500-600 DEG C; (2) bending: a hot bending glass machine is adopted; bending and forming are conducted on the pattern added glass at a hot bending temperature of 600-700 DEG C. According to the glass paint and the temperature, the glass paint can be attached to the glass well, and has excellent acidproof, alkaliproof and waterproof property; the paint is not peeled off when the glass paint is taken in secondary high-temperature heating; pai