Method for manufacturing titanium alloy oil well pipe with medium thick wall

The invention provides a method for manufacturing a titanium alloy oil well pipe with the medium thick wall. The method includes the following steps of smelting: titanium sponge is adopted, a vacuum consumable electro-arc furnace is used for smelting the titanium sponge three times, and then a phi 1...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIANG HAIQUAN, ZHANG BING, LIU JIAYONG, HOU QIANG, SUN LAIBO, ZHAO SUJUAN, LI YI, DING WEI, SUN YU, YANG YONGCHANG, WANG YAO, WANG HUIBIN, ZHANG CHUANYOU, HAO YUHUA, XIAO YAN, LI QIANG, ZHANG DANTIAN, SUN KAIMING
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention provides a method for manufacturing a titanium alloy oil well pipe with the medium thick wall. The method includes the following steps of smelting: titanium sponge is adopted, a vacuum consumable electro-arc furnace is used for smelting the titanium sponge three times, and then a phi 150mm blank pipe is forged and manufactured; heating and hole punching: the blank pipe enters an annular furnace to be heated to 980 DEG C, and the blank pipe is rolled to be a phi 152*16mm tubular billet by adopting a cone puncher; rolling: an Assel unit is adopted for rolling to reduce the thickness of the wall, the wall thickness reducing ratio is 40%, and then the phi 152*9.52mm pipe is acquired; diameter reducing: the pipe enters a reheating furnace to be heated again, then the diameter of the pipe is reduced through a 14-stand diameter reducing machine, the diameter reducing ratio is 41.5%, and then a finished pipe is acquired; thermal treatment: the punched pipe is kept at the temperature of 950-960 DEG C for