Hot melt adhesive containing modified attapulgite and preparation method thereof
The invention discloses hot melt adhesive containing modified attapulgite. The hot melt adhesive is prepared from the following components in parts by weight: 80-90 parts of EEA (eval ethylenevinyl alcohol), 10-15 parts of APAO (amorphous poly alpha olefin) ethylene-propylene-1-butene polymer, 10-12...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | FANG JUPING |
description | The invention discloses hot melt adhesive containing modified attapulgite. The hot melt adhesive is prepared from the following components in parts by weight: 80-90 parts of EEA (eval ethylenevinyl alcohol), 10-15 parts of APAO (amorphous poly alpha olefin) ethylene-propylene-1-butene polymer, 10-12 parts of epichlorohydrin rubber H75 tackifying resin, 1-2 parts of ethylene bis stearamide, 10-12 parts of modified attapulgite, 0.1-0.3 part of antioxidant 2246, 0.1-0.2 part of antioxidant DMTDP (thiodipropionate bi-tetradecyl ester), 0.2-0.3 part of antioxidant TNPP (tri-nonyl phenyl ester phosphate), 10-11 parts of acetyl triethyl citrate, and 2-3 parts of trioctyl trimellitate. The preparation method comprises the steps of: firstly preparing the epichlorohydrin rubber H75 tackifying resin, then mixing with other materials, extruding through an extruder, cooling and pelletizing. The hot melt adhesive disclosed by the invention is strong in caking property; and homemade rubber viscosity resin is added to the fo |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN103289604A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN103289604A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN103289604A3</originalsourceid><addsrcrecordid>eNqNyzEKwkAQRuFtLES9w3gAIRqRWEpQUomFfRiyf7IDm50lGT2_Fh7A6jXfW7pHo0YjohH7gFneoE6TsSRJA43qpRd4YjPOrziIgTh5yhMyT2yi6XtbUE8WMEH7tVv0HGdsfl257e36rJsdsraYM3dIsLa-74vyUJ1PxfFS_mM-0BI31A</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Hot melt adhesive containing modified attapulgite and preparation method thereof</title><source>esp@cenet</source><creator>FANG JUPING</creator><creatorcontrib>FANG JUPING</creatorcontrib><description>The invention discloses hot melt adhesive containing modified attapulgite. The hot melt adhesive is prepared from the following components in parts by weight: 80-90 parts of EEA (eval ethylenevinyl alcohol), 10-15 parts of APAO (amorphous poly alpha olefin) ethylene-propylene-1-butene polymer, 10-12 parts of epichlorohydrin rubber H75 tackifying resin, 1-2 parts of ethylene bis stearamide, 10-12 parts of modified attapulgite, 0.1-0.3 part of antioxidant 2246, 0.1-0.2 part of antioxidant DMTDP (thiodipropionate bi-tetradecyl ester), 0.2-0.3 part of antioxidant TNPP (tri-nonyl phenyl ester phosphate), 10-11 parts of acetyl triethyl citrate, and 2-3 parts of trioctyl trimellitate. The preparation method comprises the steps of: firstly preparing the epichlorohydrin rubber H75 tackifying resin, then mixing with other materials, extruding through an extruder, cooling and pelletizing. The hot melt adhesive disclosed by the invention is strong in caking property; and homemade rubber viscosity resin is added to the fo</description><language>chi ; eng</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; DYES ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; POLISHES ; PREPARATION OF CARBON BLACK ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS,TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES ; USE OF MATERIALS AS ADHESIVES</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130911&DB=EPODOC&CC=CN&NR=103289604A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130911&DB=EPODOC&CC=CN&NR=103289604A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FANG JUPING</creatorcontrib><title>Hot melt adhesive containing modified attapulgite and preparation method thereof</title><description>The invention discloses hot melt adhesive containing modified attapulgite. The hot melt adhesive is prepared from the following components in parts by weight: 80-90 parts of EEA (eval ethylenevinyl alcohol), 10-15 parts of APAO (amorphous poly alpha olefin) ethylene-propylene-1-butene polymer, 10-12 parts of epichlorohydrin rubber H75 tackifying resin, 1-2 parts of ethylene bis stearamide, 10-12 parts of modified attapulgite, 0.1-0.3 part of antioxidant 2246, 0.1-0.2 part of antioxidant DMTDP (thiodipropionate bi-tetradecyl ester), 0.2-0.3 part of antioxidant TNPP (tri-nonyl phenyl ester phosphate), 10-11 parts of acetyl triethyl citrate, and 2-3 parts of trioctyl trimellitate. The preparation method comprises the steps of: firstly preparing the epichlorohydrin rubber H75 tackifying resin, then mixing with other materials, extruding through an extruder, cooling and pelletizing. The hot melt adhesive disclosed by the invention is strong in caking property; and homemade rubber viscosity resin is added to the fo</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>DYES</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>PREPARATION OF CARBON BLACK</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS,TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyzEKwkAQRuFtLES9w3gAIRqRWEpQUomFfRiyf7IDm50lGT2_Fh7A6jXfW7pHo0YjohH7gFneoE6TsSRJA43qpRd4YjPOrziIgTh5yhMyT2yi6XtbUE8WMEH7tVv0HGdsfl257e36rJsdsraYM3dIsLa-74vyUJ1PxfFS_mM-0BI31A</recordid><startdate>20130911</startdate><enddate>20130911</enddate><creator>FANG JUPING</creator><scope>EVB</scope></search><sort><creationdate>20130911</creationdate><title>Hot melt adhesive containing modified attapulgite and preparation method thereof</title><author>FANG JUPING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN103289604A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2013</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>DYES</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>PREPARATION OF CARBON BLACK</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS,TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>FANG JUPING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FANG JUPING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Hot melt adhesive containing modified attapulgite and preparation method thereof</title><date>2013-09-11</date><risdate>2013</risdate><abstract>The invention discloses hot melt adhesive containing modified attapulgite. The hot melt adhesive is prepared from the following components in parts by weight: 80-90 parts of EEA (eval ethylenevinyl alcohol), 10-15 parts of APAO (amorphous poly alpha olefin) ethylene-propylene-1-butene polymer, 10-12 parts of epichlorohydrin rubber H75 tackifying resin, 1-2 parts of ethylene bis stearamide, 10-12 parts of modified attapulgite, 0.1-0.3 part of antioxidant 2246, 0.1-0.2 part of antioxidant DMTDP (thiodipropionate bi-tetradecyl ester), 0.2-0.3 part of antioxidant TNPP (tri-nonyl phenyl ester phosphate), 10-11 parts of acetyl triethyl citrate, and 2-3 parts of trioctyl trimellitate. The preparation method comprises the steps of: firstly preparing the epichlorohydrin rubber H75 tackifying resin, then mixing with other materials, extruding through an extruder, cooling and pelletizing. The hot melt adhesive disclosed by the invention is strong in caking property; and homemade rubber viscosity resin is added to the fo</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN103289604A |
source | esp@cenet |
subjects | ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ADHESIVES CHEMISTRY COMPOSITIONS BASED THEREON DYES MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ORGANIC MACROMOLECULAR COMPOUNDS PAINTS POLISHES PREPARATION OF CARBON BLACK THEIR PREPARATION OR CHEMICAL WORKING-UP TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS,TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES USE OF MATERIALS AS ADHESIVES |
title | Hot melt adhesive containing modified attapulgite and preparation method thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T06%3A52%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FANG%20JUPING&rft.date=2013-09-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN103289604A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |