Integrated utilization method of ironmaking dust removal ash
The invention provides an integrated utilization method of ironmaking dust removal ash, which comprises the following steps: (1) pulping; (2) carbon extraction by floatation; (3) reduction of zinc and iron; (4) water quenching and hot closed slag technique; (5) screening and crushing; (6) magnetic s...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention provides an integrated utilization method of ironmaking dust removal ash, which comprises the following steps: (1) pulping; (2) carbon extraction by floatation; (3) reduction of zinc and iron; (4) water quenching and hot closed slag technique; (5) screening and crushing; (6) magnetic separation of iron; and (7) preparation of water-permeable bricks. The grade of the regenerated carbon powder of the recovered product is 66%, and the recovery rate is 90.75%; the grade of zinc oxide is 51%, and the recovery rate is up to 76.7%; the grade of iron concentrate is 67%, and the recovery rate is 31.4%; and the grade of iron coarse ore is 36%, and the recovery rate is 14.6%. The invention can implement complete reutilization of ironmaking dust removal ash. |
---|