Soldering quality control method of large-section copper strand wire of turbonator

The invention provides a soldering quality control method of a large-section copper strand wire of a turbonator. The method is characterized in that not only the section shape of one copper wire but also the electric conductivity and the internal defects of the copper strand wire raw material are re...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GU ZHEN, CHEN GUOQIANG, ZHANG CHAOQUAN, LIN FUMIN, QUAN YUQIANG, LI BO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GU ZHEN
CHEN GUOQIANG
ZHANG CHAOQUAN
LIN FUMIN
QUAN YUQIANG
LI BO
description The invention provides a soldering quality control method of a large-section copper strand wire of a turbonator. The method is characterized in that not only the section shape of one copper wire but also the electric conductivity and the internal defects of the copper strand wire raw material are required to be controlled; after the surface of the copper strand wire is descaled, the copper strand wire is preliminarily coated with tin, joints at the ends of winding bars and jackets are preliminarily plated with silver, the plating thicknesses are larger than 10 micrometers; an induction coil is adopted for heating, the heating power is controlled to cause the temperatures of the joints to reach the soldering temperature after about one minute and thirty seconds; the difference in temperature of all positions of the joints do not exceed 50 DEG C; and the welding is finished after heating for three times. The method provided by the invention overcomes the defects in the prior art, can well control the fluctuatio
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN102983478A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN102983478A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN102983478A3</originalsourceid><addsrcrecordid>eNqNyrEKwjAQgOEsDqK-w_kABbWCdZSiODmoezmTaxuIuXi5Ir69Cj6A0z_839icLxwciY8dPAYMXl9gOapwgDtpzw64hYDSUZHJquf4-SmRQFbB6ODphb5GB7lxRGWZmlGLIdPs14mZH_bX-lhQ4oZyQkuRtKlPy8VqW5XrTbUr_zFvZAs4sg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Soldering quality control method of large-section copper strand wire of turbonator</title><source>esp@cenet</source><creator>GU ZHEN ; CHEN GUOQIANG ; ZHANG CHAOQUAN ; LIN FUMIN ; QUAN YUQIANG ; LI BO</creator><creatorcontrib>GU ZHEN ; CHEN GUOQIANG ; ZHANG CHAOQUAN ; LIN FUMIN ; QUAN YUQIANG ; LI BO</creatorcontrib><description>The invention provides a soldering quality control method of a large-section copper strand wire of a turbonator. The method is characterized in that not only the section shape of one copper wire but also the electric conductivity and the internal defects of the copper strand wire raw material are required to be controlled; after the surface of the copper strand wire is descaled, the copper strand wire is preliminarily coated with tin, joints at the ends of winding bars and jackets are preliminarily plated with silver, the plating thicknesses are larger than 10 micrometers; an induction coil is adopted for heating, the heating power is controlled to cause the temperatures of the joints to reach the soldering temperature after about one minute and thirty seconds; the difference in temperature of all positions of the joints do not exceed 50 DEG C; and the welding is finished after heating for three times. The method provided by the invention overcomes the defects in the prior art, can well control the fluctuatio</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; CLADDING OR PLATING BY SOLDERING OR WELDING ; CURRENT COLLECTORS ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; ELECTRICITY ; LINE CONNECTORS ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130320&amp;DB=EPODOC&amp;CC=CN&amp;NR=102983478A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130320&amp;DB=EPODOC&amp;CC=CN&amp;NR=102983478A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GU ZHEN</creatorcontrib><creatorcontrib>CHEN GUOQIANG</creatorcontrib><creatorcontrib>ZHANG CHAOQUAN</creatorcontrib><creatorcontrib>LIN FUMIN</creatorcontrib><creatorcontrib>QUAN YUQIANG</creatorcontrib><creatorcontrib>LI BO</creatorcontrib><title>Soldering quality control method of large-section copper strand wire of turbonator</title><description>The invention provides a soldering quality control method of a large-section copper strand wire of a turbonator. The method is characterized in that not only the section shape of one copper wire but also the electric conductivity and the internal defects of the copper strand wire raw material are required to be controlled; after the surface of the copper strand wire is descaled, the copper strand wire is preliminarily coated with tin, joints at the ends of winding bars and jackets are preliminarily plated with silver, the plating thicknesses are larger than 10 micrometers; an induction coil is adopted for heating, the heating power is controlled to cause the temperatures of the joints to reach the soldering temperature after about one minute and thirty seconds; the difference in temperature of all positions of the joints do not exceed 50 DEG C; and the welding is finished after heating for three times. The method provided by the invention overcomes the defects in the prior art, can well control the fluctuatio</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CURRENT COLLECTORS</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>ELECTRICITY</subject><subject>LINE CONNECTORS</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAQgOEsDqK-w_kABbWCdZSiODmoezmTaxuIuXi5Ir69Cj6A0z_839icLxwciY8dPAYMXl9gOapwgDtpzw64hYDSUZHJquf4-SmRQFbB6ODphb5GB7lxRGWZmlGLIdPs14mZH_bX-lhQ4oZyQkuRtKlPy8VqW5XrTbUr_zFvZAs4sg</recordid><startdate>20130320</startdate><enddate>20130320</enddate><creator>GU ZHEN</creator><creator>CHEN GUOQIANG</creator><creator>ZHANG CHAOQUAN</creator><creator>LIN FUMIN</creator><creator>QUAN YUQIANG</creator><creator>LI BO</creator><scope>EVB</scope></search><sort><creationdate>20130320</creationdate><title>Soldering quality control method of large-section copper strand wire of turbonator</title><author>GU ZHEN ; CHEN GUOQIANG ; ZHANG CHAOQUAN ; LIN FUMIN ; QUAN YUQIANG ; LI BO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN102983478A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2013</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CURRENT COLLECTORS</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>ELECTRICITY</topic><topic>LINE CONNECTORS</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>GU ZHEN</creatorcontrib><creatorcontrib>CHEN GUOQIANG</creatorcontrib><creatorcontrib>ZHANG CHAOQUAN</creatorcontrib><creatorcontrib>LIN FUMIN</creatorcontrib><creatorcontrib>QUAN YUQIANG</creatorcontrib><creatorcontrib>LI BO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GU ZHEN</au><au>CHEN GUOQIANG</au><au>ZHANG CHAOQUAN</au><au>LIN FUMIN</au><au>QUAN YUQIANG</au><au>LI BO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Soldering quality control method of large-section copper strand wire of turbonator</title><date>2013-03-20</date><risdate>2013</risdate><abstract>The invention provides a soldering quality control method of a large-section copper strand wire of a turbonator. The method is characterized in that not only the section shape of one copper wire but also the electric conductivity and the internal defects of the copper strand wire raw material are required to be controlled; after the surface of the copper strand wire is descaled, the copper strand wire is preliminarily coated with tin, joints at the ends of winding bars and jackets are preliminarily plated with silver, the plating thicknesses are larger than 10 micrometers; an induction coil is adopted for heating, the heating power is controlled to cause the temperatures of the joints to reach the soldering temperature after about one minute and thirty seconds; the difference in temperature of all positions of the joints do not exceed 50 DEG C; and the welding is finished after heating for three times. The method provided by the invention overcomes the defects in the prior art, can well control the fluctuatio</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN102983478A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CLADDING OR PLATING BY SOLDERING OR WELDING
CURRENT COLLECTORS
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
ELECTRICITY
LINE CONNECTORS
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title Soldering quality control method of large-section copper strand wire of turbonator
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-10T14%3A37%3A27IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GU%20ZHEN&rft.date=2013-03-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN102983478A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true