High-performance rare earth permanent magnet sintered magnet and manufacturing method thereof
The invention provides a rare earth sintered magnet and a manufacturing method thereof. The magnetic property residual magnetism Br of the magnet is between 12.8 and 13.3 kGs, the intrinsic coercivity Hcj is more than or equal to 30 kOe, and the content of oxygen in the magnet is between 500 and 900...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention provides a rare earth sintered magnet and a manufacturing method thereof. The magnetic property residual magnetism Br of the magnet is between 12.8 and 13.3 kGs, the intrinsic coercivity Hcj is more than or equal to 30 kOe, and the content of oxygen in the magnet is between 500 and 900 ppm. The rare earth sintered magnet is prepared by the manufacturing process that: a smelting procedure is a vacuum quick-setting process, and the thickness of produced sheet alloys is between 0.1 and 0.5mm; a hydrogen decrepitation process is used for production in an intermediate crushing procedure; a jet mill is used for production in a micro powder manufacturing procedure, and the average particle size of micro powder is between 3.0 and 4.5 mu m; a compression procedure is used for compression molding under the environment of anaerobic inert gas; and a sintering procedure is used for sintering and aging by means of a vacuum sintering furnace. |
---|