Method for preparing meta-aramid fiber

The invention discloses a method for preparing meta-aramid fiber. The method comprises the following steps of: adding meta-phenylene diamine into a polar solvent; reducing the temperature to be between -10 DEG C and 10 DEG C; gradually adding meta-phthaloyl chloride for reaction; regulating the pH o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SONG XIQUAN, LV JIPING, PAN SHIDONG, SONG CUIYAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SONG XIQUAN
LV JIPING
PAN SHIDONG
SONG CUIYAN
description The invention discloses a method for preparing meta-aramid fiber. The method comprises the following steps of: adding meta-phenylene diamine into a polar solvent; reducing the temperature to be between -10 DEG C and 10 DEG C; gradually adding meta-phthaloyl chloride for reaction; regulating the pH of a reaction solution to be neutral after the reaction; filtering to obtain a spinning solution; heating the spinning solution to the temperature of between 50 DEG C and 120 DEG C; ejecting the spinning solution into a channel through a spinning plate; and removing the solvent in the fiber through a gaseous medium in the channel, and solidifying and molding the fiber to obtain as-spun fiber; soaking the as-spun fiber in a mixed solution of water and organic solvents for certain time; and performing water-washing drawing, drying, molding after heat treatment, cooling and oiling to obtain the meta-aramid fiber. The method for preparing the meta-aramid fiber has the advantages of high spinning speed, and high quality
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN102534839A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN102534839A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN102534839A3</originalsourceid><addsrcrecordid>eNrjZFDzTS3JyE9RSMsvUigoSi1ILMrMS1fITS1J1E0sSszNBMpkJqUW8TCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_QwMjU2MTC2NLR2Ni1AAAVKwnTQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing meta-aramid fiber</title><source>esp@cenet</source><creator>SONG XIQUAN ; LV JIPING ; PAN SHIDONG ; SONG CUIYAN</creator><creatorcontrib>SONG XIQUAN ; LV JIPING ; PAN SHIDONG ; SONG CUIYAN</creatorcontrib><description>The invention discloses a method for preparing meta-aramid fiber. The method comprises the following steps of: adding meta-phenylene diamine into a polar solvent; reducing the temperature to be between -10 DEG C and 10 DEG C; gradually adding meta-phthaloyl chloride for reaction; regulating the pH of a reaction solution to be neutral after the reaction; filtering to obtain a spinning solution; heating the spinning solution to the temperature of between 50 DEG C and 120 DEG C; ejecting the spinning solution into a channel through a spinning plate; and removing the solvent in the fiber through a gaseous medium in the channel, and solidifying and molding the fiber to obtain as-spun fiber; soaking the as-spun fiber in a mixed solution of water and organic solvents for certain time; and performing water-washing drawing, drying, molding after heat treatment, cooling and oiling to obtain the meta-aramid fiber. The method for preparing the meta-aramid fiber has the advantages of high spinning speed, and high quality</description><language>chi ; eng</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS ; METALLURGY ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; ORGANIC MACROMOLECULAR COMPOUNDS ; SPINNING ; TEXTILES ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120704&amp;DB=EPODOC&amp;CC=CN&amp;NR=102534839A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120704&amp;DB=EPODOC&amp;CC=CN&amp;NR=102534839A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SONG XIQUAN</creatorcontrib><creatorcontrib>LV JIPING</creatorcontrib><creatorcontrib>PAN SHIDONG</creatorcontrib><creatorcontrib>SONG CUIYAN</creatorcontrib><title>Method for preparing meta-aramid fiber</title><description>The invention discloses a method for preparing meta-aramid fiber. The method comprises the following steps of: adding meta-phenylene diamine into a polar solvent; reducing the temperature to be between -10 DEG C and 10 DEG C; gradually adding meta-phthaloyl chloride for reaction; regulating the pH of a reaction solution to be neutral after the reaction; filtering to obtain a spinning solution; heating the spinning solution to the temperature of between 50 DEG C and 120 DEG C; ejecting the spinning solution into a channel through a spinning plate; and removing the solvent in the fiber through a gaseous medium in the channel, and solidifying and molding the fiber to obtain as-spun fiber; soaking the as-spun fiber in a mixed solution of water and organic solvents for certain time; and performing water-washing drawing, drying, molding after heat treatment, cooling and oiling to obtain the meta-aramid fiber. The method for preparing the meta-aramid fiber has the advantages of high spinning speed, and high quality</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS</subject><subject>METALLURGY</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>SPINNING</subject><subject>TEXTILES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFDzTS3JyE9RSMsvUigoSi1ILMrMS1fITS1J1E0sSszNBMpkJqUW8TCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_QwMjU2MTC2NLR2Ni1AAAVKwnTQ</recordid><startdate>20120704</startdate><enddate>20120704</enddate><creator>SONG XIQUAN</creator><creator>LV JIPING</creator><creator>PAN SHIDONG</creator><creator>SONG CUIYAN</creator><scope>EVB</scope></search><sort><creationdate>20120704</creationdate><title>Method for preparing meta-aramid fiber</title><author>SONG XIQUAN ; LV JIPING ; PAN SHIDONG ; SONG CUIYAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN102534839A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2012</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS</topic><topic>METALLURGY</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>SPINNING</topic><topic>TEXTILES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>SONG XIQUAN</creatorcontrib><creatorcontrib>LV JIPING</creatorcontrib><creatorcontrib>PAN SHIDONG</creatorcontrib><creatorcontrib>SONG CUIYAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SONG XIQUAN</au><au>LV JIPING</au><au>PAN SHIDONG</au><au>SONG CUIYAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing meta-aramid fiber</title><date>2012-07-04</date><risdate>2012</risdate><abstract>The invention discloses a method for preparing meta-aramid fiber. The method comprises the following steps of: adding meta-phenylene diamine into a polar solvent; reducing the temperature to be between -10 DEG C and 10 DEG C; gradually adding meta-phthaloyl chloride for reaction; regulating the pH of a reaction solution to be neutral after the reaction; filtering to obtain a spinning solution; heating the spinning solution to the temperature of between 50 DEG C and 120 DEG C; ejecting the spinning solution into a channel through a spinning plate; and removing the solvent in the fiber through a gaseous medium in the channel, and solidifying and molding the fiber to obtain as-spun fiber; soaking the as-spun fiber in a mixed solution of water and organic solvents for certain time; and performing water-washing drawing, drying, molding after heat treatment, cooling and oiling to obtain the meta-aramid fiber. The method for preparing the meta-aramid fiber has the advantages of high spinning speed, and high quality</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN102534839A
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS
METALLURGY
NATURAL OR ARTIFICIAL THREADS OR FIBRES
ORGANIC MACROMOLECULAR COMPOUNDS
SPINNING
TEXTILES
THEIR PREPARATION OR CHEMICAL WORKING-UP
title Method for preparing meta-aramid fiber
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-15T07%3A29%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SONG%20XIQUAN&rft.date=2012-07-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN102534839A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true