Method for treating steel for directional electromagnetic steel plate and method for producing directional electromagnetic steel plate

The surface temperature of a slab is reduced so as not to exceed 600 DEG C from the start of the continuous casting (step S2) to the start of the slab reheating (step S3). The surface temperature of the slab is maintained at a temperature of at least 150 DEG C from the start of continuous casting (s...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YAMAMOTO NORIHIRO, USHIGAMI YOSHIYUKI, KUMANO TOMOJI, NAKAMURA SYUUICHI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The surface temperature of a slab is reduced so as not to exceed 600 DEG C from the start of the continuous casting (step S2) to the start of the slab reheating (step S3). The surface temperature of the slab is maintained at a temperature of at least 150 DEG C from the start of continuous casting (step S2) to the start of slab reheating (S3). The surface temperature of the slab during slab reheating (step S3) is maintained between 1080 DEG C and 1200 DEG C.