Processing method of foaming polyurethane and volume reduction processing device of foaming polyurethane
PROBLEM TO BE SOLVED: To continuously process a waste of bulky foamed polyurethane, which is compressed into a high density.SOLUTION: A method includes the steps of: heating the foamed polyurethane; applying a shearing force thereto for pressurization; and reducing the volume by the compression of t...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To continuously process a waste of bulky foamed polyurethane, which is compressed into a high density.SOLUTION: A method includes the steps of: heating the foamed polyurethane; applying a shearing force thereto for pressurization; and reducing the volume by the compression of the foamed polyurethane. Thereby, the density of the foamed polyurethane is increased. Preferably, a screw extruder may be used. |
---|