Porous magnesia clinker, manufacturing method and use thereof as flux for treating steelmaking slag
A clinker composition including, relative to the clinker total weight: from 30 to 85% Al2O3; from 3 to 45% CaO; from 9 to 45% MgO and having an apparent porosity, such as measured by means of the apparent porosity underwater measurement assay according to modified NF B40-312 standard ranging from 4%...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A clinker composition including, relative to the clinker total weight: from 30 to 85% Al2O3; from 3 to 45% CaO; from 9 to 45% MgO and having an apparent porosity, such as measured by means of the apparent porosity underwater measurement assay according to modified NF B40-312 standard ranging from 4% to 60%. |
---|