Quick reparation method for heteroatom phosphorus aluminum molecular sieve in eutectoid
The invention discloses a quick reparation method for a heteroatom phosphorus aluminum molecular sieve in eutectoid. The method comprises the following steps of: (1) mixing the eutectoid, an aluminum source and an iron source uniformly, and adding phosphoric acid and pyridine, wherein the formed mix...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WANG HUA KANG CHUNXI LUO CUIHONG ZHAO XINHONG |
description | The invention discloses a quick reparation method for a heteroatom phosphorus aluminum molecular sieve in eutectoid. The method comprises the following steps of: (1) mixing the eutectoid, an aluminum source and an iron source uniformly, and adding phosphoric acid and pyridine, wherein the formed mixture is aFe2O3:Al2O3:bP2O5:cC5H5N:d eutectoid, and in molar ratio, a is 2.0 to 3.0, b is 2.5 to 3.0, c is 3.5 to 4.0 and d is 55.0 to 60.0; mixing the mixture uniformly with heating at the temperature of between 50 and 80 DEG C; (2) heating the mixture to the temperature of between 150 and 220 DEG C under microwave radiation, and crystallizing the mixture for 20 to 60 minutes under normal pressure or automatic generated pressure; and (3) cooling the crystallized mixture to room temperature, performing vacuum filtration, repeatedly washing the filtered product by using water and acetone, and drying the washed product at the temperature o between 80 and 100 DEG C to obtain a powdery product of the heteroatom phosphor |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN102153106A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN102153106A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN102153106A3</originalsourceid><addsrcrecordid>eNqNyjEKAjEQRuE0FqLeYTyAsOuivSyKlSAIlsuQ_ZcNJpmQTDy_Fh7A4vE1b2me9-rsizISZ1YnkQJ0lpEmyTRDkYVVAqVZyrdcC7GvwcUaKIiHrZ4zFYc3yEVCVVgVN67NYmJfsPm5MtvL-dFfd0gyoCS2iNChv7XNvj10bXM8df88H-BoOtY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Quick reparation method for heteroatom phosphorus aluminum molecular sieve in eutectoid</title><source>esp@cenet</source><creator>WANG HUA ; KANG CHUNXI ; LUO CUIHONG ; ZHAO XINHONG</creator><creatorcontrib>WANG HUA ; KANG CHUNXI ; LUO CUIHONG ; ZHAO XINHONG</creatorcontrib><description>The invention discloses a quick reparation method for a heteroatom phosphorus aluminum molecular sieve in eutectoid. The method comprises the following steps of: (1) mixing the eutectoid, an aluminum source and an iron source uniformly, and adding phosphoric acid and pyridine, wherein the formed mixture is aFe2O3:Al2O3:bP2O5:cC5H5N:d eutectoid, and in molar ratio, a is 2.0 to 3.0, b is 2.5 to 3.0, c is 3.5 to 4.0 and d is 55.0 to 60.0; mixing the mixture uniformly with heating at the temperature of between 50 and 80 DEG C; (2) heating the mixture to the temperature of between 150 and 220 DEG C under microwave radiation, and crystallizing the mixture for 20 to 60 minutes under normal pressure or automatic generated pressure; and (3) cooling the crystallized mixture to room temperature, performing vacuum filtration, repeatedly washing the filtered product by using water and acetone, and drying the washed product at the temperature o between 80 and 100 DEG C to obtain a powdery product of the heteroatom phosphor</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2011</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20110817&DB=EPODOC&CC=CN&NR=102153106A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20110817&DB=EPODOC&CC=CN&NR=102153106A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG HUA</creatorcontrib><creatorcontrib>KANG CHUNXI</creatorcontrib><creatorcontrib>LUO CUIHONG</creatorcontrib><creatorcontrib>ZHAO XINHONG</creatorcontrib><title>Quick reparation method for heteroatom phosphorus aluminum molecular sieve in eutectoid</title><description>The invention discloses a quick reparation method for a heteroatom phosphorus aluminum molecular sieve in eutectoid. The method comprises the following steps of: (1) mixing the eutectoid, an aluminum source and an iron source uniformly, and adding phosphoric acid and pyridine, wherein the formed mixture is aFe2O3:Al2O3:bP2O5:cC5H5N:d eutectoid, and in molar ratio, a is 2.0 to 3.0, b is 2.5 to 3.0, c is 3.5 to 4.0 and d is 55.0 to 60.0; mixing the mixture uniformly with heating at the temperature of between 50 and 80 DEG C; (2) heating the mixture to the temperature of between 150 and 220 DEG C under microwave radiation, and crystallizing the mixture for 20 to 60 minutes under normal pressure or automatic generated pressure; and (3) cooling the crystallized mixture to room temperature, performing vacuum filtration, repeatedly washing the filtered product by using water and acetone, and drying the washed product at the temperature o between 80 and 100 DEG C to obtain a powdery product of the heteroatom phosphor</description><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2011</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEKAjEQRuE0FqLeYTyAsOuivSyKlSAIlsuQ_ZcNJpmQTDy_Fh7A4vE1b2me9-rsizISZ1YnkQJ0lpEmyTRDkYVVAqVZyrdcC7GvwcUaKIiHrZ4zFYc3yEVCVVgVN67NYmJfsPm5MtvL-dFfd0gyoCS2iNChv7XNvj10bXM8df88H-BoOtY</recordid><startdate>20110817</startdate><enddate>20110817</enddate><creator>WANG HUA</creator><creator>KANG CHUNXI</creator><creator>LUO CUIHONG</creator><creator>ZHAO XINHONG</creator><scope>EVB</scope></search><sort><creationdate>20110817</creationdate><title>Quick reparation method for heteroatom phosphorus aluminum molecular sieve in eutectoid</title><author>WANG HUA ; KANG CHUNXI ; LUO CUIHONG ; ZHAO XINHONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN102153106A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2011</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG HUA</creatorcontrib><creatorcontrib>KANG CHUNXI</creatorcontrib><creatorcontrib>LUO CUIHONG</creatorcontrib><creatorcontrib>ZHAO XINHONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG HUA</au><au>KANG CHUNXI</au><au>LUO CUIHONG</au><au>ZHAO XINHONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Quick reparation method for heteroatom phosphorus aluminum molecular sieve in eutectoid</title><date>2011-08-17</date><risdate>2011</risdate><abstract>The invention discloses a quick reparation method for a heteroatom phosphorus aluminum molecular sieve in eutectoid. The method comprises the following steps of: (1) mixing the eutectoid, an aluminum source and an iron source uniformly, and adding phosphoric acid and pyridine, wherein the formed mixture is aFe2O3:Al2O3:bP2O5:cC5H5N:d eutectoid, and in molar ratio, a is 2.0 to 3.0, b is 2.5 to 3.0, c is 3.5 to 4.0 and d is 55.0 to 60.0; mixing the mixture uniformly with heating at the temperature of between 50 and 80 DEG C; (2) heating the mixture to the temperature of between 150 and 220 DEG C under microwave radiation, and crystallizing the mixture for 20 to 60 minutes under normal pressure or automatic generated pressure; and (3) cooling the crystallized mixture to room temperature, performing vacuum filtration, repeatedly washing the filtered product by using water and acetone, and drying the washed product at the temperature o between 80 and 100 DEG C to obtain a powdery product of the heteroatom phosphor</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN102153106A |
source | esp@cenet |
subjects | CHEMISTRY COMPOUNDS THEREOF INORGANIC CHEMISTRY METALLURGY NON-METALLIC ELEMENTS |
title | Quick reparation method for heteroatom phosphorus aluminum molecular sieve in eutectoid |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T07%3A13%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20HUA&rft.date=2011-08-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN102153106A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |