Modified Y type molecular sieve/matrix composite material and preparation method thereof

The invention relates to a modified in-situ crystallization Y type molecular sieve/matrix composite material, the surface of which is loaded with 0.001 to 5.0% by weight of RE2O3, 0 to 3.0% by weight of SiO2, 0 to 3.0% by weight of Al2O3 and 0 to 3.0% by weight of MgO. The composite material is prep...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG YULIANG, ZHANG LING, LU SHANXIANG, JIANG DECHAO, LEI FANGFANG, FENG SHUILI, CHEN HUI, SU QIONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a modified in-situ crystallization Y type molecular sieve/matrix composite material, the surface of which is loaded with 0.001 to 5.0% by weight of RE2O3, 0 to 3.0% by weight of SiO2, 0 to 3.0% by weight of Al2O3 and 0 to 3.0% by weight of MgO. The composite material is prepared by adjusting pH of kaolin in-situ crystallization Y type molecular sieve/matrix material to 8-11 by using a solution containing one or more of soluble glass, sodium metaaluminate and magnesium hydroxide, or ammonia water in separate steps or in combination after ammonium exchange and/or rare earth exchange, stirring, filtering, washing, drying, roasting and exchanging with ammonium.