Oil-soluble thick oil yield increasing and viscosity reducing agent and preparation

The invention provides an oil-soluble thick oil yield increasing and viscosity reducing agent and preparation. The oil-soluble thick oil yield increasing and viscosity reducing agent is prepared from the following ingredients in parts by weight: 10 to 20 parts of acrylic acid higher-alcohol ester st...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SUN CHAN, LIU HUANJIANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention provides an oil-soluble thick oil yield increasing and viscosity reducing agent and preparation. The oil-soluble thick oil yield increasing and viscosity reducing agent is prepared from the following ingredients in parts by weight: 10 to 20 parts of acrylic acid higher-alcohol ester styrol copolymer, 5 to 8 parts of ketone, 10 to 20 parts of random polyether, 5 to 10 parts of glycoland 42 to 70 parts of organic solvents. The preparation method comprises the following steps of: sequentially adding the organic solvent, the ketone, the glycol and the random polyether to a reactionkettle, then, adding the acrylic acid higher-alcohol ester styrol copolymer under the stirring condition at 35 to 45 DEG C, controlling the temperature for 25 to 35 minutes, and uniformly stirring toobtain the product. The acrylic acid higher-alcohol ester styrol copolymer is adopted as an acrylic acid 12-18 alcohol ester styrol copolymer, the adopted ketone is acetone, cyclohexanone, 2-heptanone, ethyl methyl ketone, isop