Recovery process of low-grade oxidizing molybdenum ore

The invention discloses a recovery process of low-grade oxidizing molybdenum ore, belonging to the technical filed of metallurgy and comprising the following steps of: crushing, grinding and preliminarily floating ore in sequence; leaching rough concentrate obtained by preliminary floating with alka...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG QINGLI, LIU HAIGE, FAN SHANGLI, KU JIANGANG, WANG ANLI, CAI SHENGFENG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses a recovery process of low-grade oxidizing molybdenum ore, belonging to the technical filed of metallurgy and comprising the following steps of: crushing, grinding and preliminarily floating ore in sequence; leaching rough concentrate obtained by preliminary floating with alkaline; obtaining alkaline leaching slag and a molybdate-containing precious solution by solid-liquidseparation after alkaline leaching; secondarily floating alkaline leaching slag to obtain molybdenum concentrate; and transferring the molybdate-containing precious solution to ammonium molybdate forproduction. During preliminary floating, the ore pulp density is 30-35 percent and a floating medicine is lime, copper sulfate, sodium sulfide, water glass, sodium butyl xanthogenate, SN-9, kerosene and No.2 oil. With the technical scheme, the molybdenum ore with the oxygenation efficiency of 50-90 percent and the molybdenum grade of 0.08-0.5 percent can be treated to obtain the rough molybdeniteconcentrate with the molybd