Preparing method of ceram site fully using biosolid and sludge

This invention discloses a preparing method of ceram site fully using biosolid and sludge, including steps as follows: a, mixing materials; b, preparing particles; c, sintering at temperature of 1000-1300 degrees centigrade after pre-heating for 5-20 minutes; cooling at temperature of 50-200 degrees...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG XIAOHUA, TIAN SHENGCHUN, TONG LIMEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This invention discloses a preparing method of ceram site fully using biosolid and sludge, including steps as follows: a, mixing materials; b, preparing particles; c, sintering at temperature of 1000-1300 degrees centigrade after pre-heating for 5-20 minutes; cooling at temperature of 50-200 degrees centigrade for 10-30 minutes after sintering, thereby preparing finished ceram site product. Accordingly, this invention makes effective use of urban mud, and changes industrial waste solid into valuable; further, this utilyit model is low in preparation cost and suitable for large-scaled production.