Method for producing large thickness and high intensity steel plate for boiler drum

The invention discloses a production method for a high tensile steel plate used for a high thickness boiler drum. The production method comprises the following steps: (1) smelting: smelting molten steel in an electric furnace, the refining the molten steel in an LF finer, adding 300 to 500 meters of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YU SHENG, SONG XIANGQIAN, NING KANGKANG, ZHAO QUANQING, LI JINGTAO, HE GUANGXIA, REN JUNKUI, LUO JUNGAO, QI YAN, CHEN JUNQI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses a production method for a high tensile steel plate used for a high thickness boiler drum. The production method comprises the following steps: (1) smelting: smelting molten steel in an electric furnace, the refining the molten steel in an LF finer, adding 300 to 500 meters of Al thread, and carrying out vacuum treatment in a bale VD furnace when the temperature of the baleis more than or equal to 1600 DEG C; (2) casting: keeping the temperature between 1,545 and 1,555 DEG C after damaging the vacuum; (3) heating: realizing the sending, clearing and filling of a steel ingot at a moderate temperature, cooling down the furnace for over 30 minutes before steel filling, and stewing the steel for one hour; (4) rolling: adopting II type rolling control technology, and setting a first stage as an austenite recrystallization stage and a second stage as an austenite non-recrystallization stage; (5) water cooling: cooling down the rolled steel plate on line, and keeping the red temperature betwee