Method for preparing protecting residue from recovery refining slag

The invention relates to a method for preparing protecting slag from recovered refining slag remained in a ladle after continuous casting, which is characterized in that the recovered refining slag is natural cooled down, pulverized, subjected to iron removal and passes a 80-mesh screen; undersize i...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: XIE JIAN, YIN YUFU, TANG ZHIKUI, ZHANG XINGHUA, LI JIE, HUANG FENG, WU YONGLAI, YANG ZHENGHONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a method for preparing protecting slag from recovered refining slag remained in a ladle after continuous casting, which is characterized in that the recovered refining slag is natural cooled down, pulverized, subjected to iron removal and passes a 80-mesh screen; undersize is picked up and subjected to component analysis; according to the target component of the prepared protecting slag, if corresponding amount of natural mineral or fine powder of manually synthesized material containing the lacked components needs to be added, butane radical sodium xanthate and balling bonding agent in the general adding amount are added to prepare pulp with the solid content of between 50 and 70 weight percent, and the pulp is sprayed at the tower top at a hot air temperature ofbetween 550 and 650 DEG C to prepare hollow micro balls. The invention has two characteristics: 1. the method has the simple recycling process, and the materials used to prepared the protecting slag are calculated and added o