Process of preparing high-performance magnetism temperature compensation alloy for gyroscope
The invention discloses a preparing craft of gyroscopic instrument permanent-magnet torque device with magnetic temperature to compensate alloy, which comprises the following steps: adopting powder metallurgic method to produce magnet temperature compensation alloy; pressing the mixing powder at the...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | XUANHUI,LI QU |
description | The invention discloses a preparing craft of gyroscopic instrument permanent-magnet torque device with magnetic temperature to compensate alloy, which comprises the following steps: adopting powder metallurgic method to produce magnet temperature compensation alloy; pressing the mixing powder at the pressure of 100-200MPa; clinkering with hard vacuum furnace; setting the vacuum degree at 1X10-3Pa-1X10-2Pa, clinkering temperature at 1200-1380 deg.c and keeping time at 2-8 h; cooling; controlling the temperature between 200 deg.c and room temperature; tapping; getting the product. This invention possesses merits of big stability, strong compensatory capacity, small DeltaB/DeltaT value fluctuation, good compatibility and DeltaB/DeltaT=0.0054-0.0055T/deg.C at the same time. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN101016593A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN101016593A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN101016593A3</originalsourceid><addsrcrecordid>eNqNjLEKAjEQRNNYiPoP6wccKIeC5XEoVmJhKRxL2OQCSTbsxuL-3hR-gEwxA29m1ub9FLakCuygCBWUkD3Mwc9dIXEsCbMlSOgz1aAJKqUGsH6EwHLLWbEGzoAx8gJtAX4RVsuFtmblMCrtfr4x-9v1Nd47KjyRFrTUXqfxcTw0nU-Xfuj_6XwBRII8-A</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Process of preparing high-performance magnetism temperature compensation alloy for gyroscope</title><source>esp@cenet</source><creator>XUANHUI,LI QU</creator><creatorcontrib>XUANHUI,LI QU</creatorcontrib><description>The invention discloses a preparing craft of gyroscopic instrument permanent-magnet torque device with magnetic temperature to compensate alloy, which comprises the following steps: adopting powder metallurgic method to produce magnet temperature compensation alloy; pressing the mixing powder at the pressure of 100-200MPa; clinkering with hard vacuum furnace; setting the vacuum degree at 1X10-3Pa-1X10-2Pa, clinkering temperature at 1200-1380 deg.c and keeping time at 2-8 h; cooling; controlling the temperature between 200 deg.c and room temperature; tapping; getting the product. This invention possesses merits of big stability, strong compensatory capacity, small DeltaB/DeltaT value fluctuation, good compatibility and DeltaB/DeltaT=0.0054-0.0055T/deg.C at the same time.</description><language>eng</language><subject>ALLOYS ; CASTING ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; MAKING METALLIC POWDER ; MANUFACTURE OF ARTICLES FROM METALLIC POWDER ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS ; WORKING METALLIC POWDER</subject><creationdate>2007</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20070815&DB=EPODOC&CC=CN&NR=101016593A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20070815&DB=EPODOC&CC=CN&NR=101016593A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>XUANHUI,LI QU</creatorcontrib><title>Process of preparing high-performance magnetism temperature compensation alloy for gyroscope</title><description>The invention discloses a preparing craft of gyroscopic instrument permanent-magnet torque device with magnetic temperature to compensate alloy, which comprises the following steps: adopting powder metallurgic method to produce magnet temperature compensation alloy; pressing the mixing powder at the pressure of 100-200MPa; clinkering with hard vacuum furnace; setting the vacuum degree at 1X10-3Pa-1X10-2Pa, clinkering temperature at 1200-1380 deg.c and keeping time at 2-8 h; cooling; controlling the temperature between 200 deg.c and room temperature; tapping; getting the product. This invention possesses merits of big stability, strong compensatory capacity, small DeltaB/DeltaT value fluctuation, good compatibility and DeltaB/DeltaT=0.0054-0.0055T/deg.C at the same time.</description><subject>ALLOYS</subject><subject>CASTING</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>MAKING METALLIC POWDER</subject><subject>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><subject>WORKING METALLIC POWDER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2007</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLEKAjEQRNNYiPoP6wccKIeC5XEoVmJhKRxL2OQCSTbsxuL-3hR-gEwxA29m1ub9FLakCuygCBWUkD3Mwc9dIXEsCbMlSOgz1aAJKqUGsH6EwHLLWbEGzoAx8gJtAX4RVsuFtmblMCrtfr4x-9v1Nd47KjyRFrTUXqfxcTw0nU-Xfuj_6XwBRII8-A</recordid><startdate>20070815</startdate><enddate>20070815</enddate><creator>XUANHUI,LI QU</creator><scope>EVB</scope></search><sort><creationdate>20070815</creationdate><title>Process of preparing high-performance magnetism temperature compensation alloy for gyroscope</title><author>XUANHUI,LI QU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN101016593A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2007</creationdate><topic>ALLOYS</topic><topic>CASTING</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>MAKING METALLIC POWDER</topic><topic>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><topic>WORKING METALLIC POWDER</topic><toplevel>online_resources</toplevel><creatorcontrib>XUANHUI,LI QU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>XUANHUI,LI QU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Process of preparing high-performance magnetism temperature compensation alloy for gyroscope</title><date>2007-08-15</date><risdate>2007</risdate><abstract>The invention discloses a preparing craft of gyroscopic instrument permanent-magnet torque device with magnetic temperature to compensate alloy, which comprises the following steps: adopting powder metallurgic method to produce magnet temperature compensation alloy; pressing the mixing powder at the pressure of 100-200MPa; clinkering with hard vacuum furnace; setting the vacuum degree at 1X10-3Pa-1X10-2Pa, clinkering temperature at 1200-1380 deg.c and keeping time at 2-8 h; cooling; controlling the temperature between 200 deg.c and room temperature; tapping; getting the product. This invention possesses merits of big stability, strong compensatory capacity, small DeltaB/DeltaT value fluctuation, good compatibility and DeltaB/DeltaT=0.0054-0.0055T/deg.C at the same time.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_CN101016593A |
source | esp@cenet |
subjects | ALLOYS CASTING CHEMISTRY FERROUS OR NON-FERROUS ALLOYS MAKING METALLIC POWDER MANUFACTURE OF ARTICLES FROM METALLIC POWDER METALLURGY PERFORMING OPERATIONS POWDER METALLURGY TRANSPORTING TREATMENT OF ALLOYS OR NON-FERROUS METALS WORKING METALLIC POWDER |
title | Process of preparing high-performance magnetism temperature compensation alloy for gyroscope |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T11%3A47%3A34IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=XUANHUI,LI%20QU&rft.date=2007-08-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN101016593A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |