The current invention is directed to a process to sinter an ultra high molecular weight polyethylene (UHMW-PE) having a weight average molecular mass of more than 1.10 g/mol, wherein a disentangled UHMW-PE is heated to a temperature above its equilibrium melting temperature at a pressure below 20 MP...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The current invention is directed to a process to sinter an ultra high molecular weight polyethylene (UHMW-PE) having a weight average molecular mass of more than 1.10 g/mol, wherein a disentangled UHMW-PE is heated to a temperature above its equilibrium melting temperature at a pressure below 20 MPa. |
---|