Procedimiento para recuperar metales no ferrosos de matriz solida, que comprende lixiviar la matriz con una solucion de base acuosa que contiene iones de cloruro e iones de amonio y que tiene un ph entre 6,5 y 8,5, en presencia de oxigeno

A process for recovering non-ferrous metals from a solid matrix may include: (a) leaching the solid matrix with an aqueous-based solution containing chloride ions, ammonium ions, and Cu2+ ions, having a pH of 6.5-8.5, in a presence of oxygen, at a temperature of 100° C.-160° C. and a pressure of 150...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LANE, WILLIAM LEONARD, HYMER TIMOTHY ROY, NIELSEN JONATHAN HYLKJIER, OLKKOMEN DAVID MICHAEL, MACCAGNI MASSIMO GIUSEPPE
Format: Patent
Sprache:spa
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A process for recovering non-ferrous metals from a solid matrix may include: (a) leaching the solid matrix with an aqueous-based solution containing chloride ions, ammonium ions, and Cu2+ ions, having a pH of 6.5-8.5, in a presence of oxygen, at a temperature of 100° C.-160° C. and a pressure of 150 kPa-800 kPa, so as to obtain an extraction solution comprising leached metals and solid leaching residue; (b) separating the solid leaching residue from the extraction solution; and/or (c) subjecting the extraction solution to at least one cementation so as to recover the leached metals in elemental state. The pH may be greater than or equal to 6.5 and less than or equal to 8.5. Temperature may be greater than or equal to 100° C. and less than or equal to 160° C. Pressure may be greater than or equal to 150 kPa and less than or equal to 800 kPa.