BIMODAL POLYETHYLENE RESINS AND PIPES PRODUCED THEREFROM

Disclosed herein are ethylene-based polymers generally characterized by a density of at least 0.94 g/cm3, a high load melt index from 4 to 20 g/10 min, a zero-shear viscosity at 190 oC from 20,000 to 400,000 kPa-sec, and a relaxation time at 190 oC from 225 to 3000 sec. These ethylene polymers can b...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LANIER, ELIZABETH M, SUKHADIA, ASHISH M, INN, YONGWOO, ROHATGI, VIVEK
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Disclosed herein are ethylene-based polymers generally characterized by a density of at least 0.94 g/cm3, a high load melt index from 4 to 20 g/10 min, a zero-shear viscosity at 190 oC from 20,000 to 400,000 kPa-sec, and a relaxation time at 190 oC from 225 to 3000 sec. These ethylene polymers can be produced by peroxide-treating a broad molecular weight distribution Ziegler-catalyzed resin, and can be used in large diameter, thick wall pipes and other end-use applications. L'invention concerne des polymères à base d'éthylène caractérisés généralement par une densité d'au moins 0,94 g/3, un indice de fusion à charge élevée de 4 à 20 g/10 min, une viscosité à cisaillement nul à 190 oC de 20 000 à 400 000 kPa-Sec, et un temps de relaxation à 190 oC de 225 à 3 000 sec. Ces polymères d'éthylène peuvent être produits par traitement au peroxyde d'une résine ayant subie une catalyse de Ziegler à large distribution de poids moléculaire, et peuvent être utilisés dans des tuyaux de grand diamètre à paroi épaisse et d'autres applications d'utilisation finale.