WELDING MATERIAL FOR WELDING OF SUPERALLOYS
Welding material for welding of superalloys comprising boron with the range of 0.3 - 0.8 wt. % B, 0.2 - 0.8 wt. % C, 17 - 23 wt. % Cr, 0.35 - 10 wt. % Mo, 0.1 - 4.15 wt. % Nb with nickel or iron and impurities to balance for weld repair of engine components manufactured of precipitation hardening su...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Welding material for welding of superalloys comprising boron with the range of 0.3 - 0.8 wt. % B, 0.2 - 0.8 wt. % C, 17 - 23 wt. % Cr, 0.35 - 10 wt. % Mo, 0.1 - 4.15 wt. % Nb with nickel or iron and impurities to balance for weld repair of engine components manufactured of precipitation hardening superalloys with high content of gamma prime phase at an ambient temperature. |
---|