IRON-BASE ALLOY AND METHOD FOR PRODUCING THE SAME

An iron-based alloy comprises 1.5 to 2.5 wt% of C, 0.25 to 4.75 wt% of Ni, and W and V in quantities surrounded by the line L as shown in Fig. 1 of the attached drawings with a balance of Fe and inevitable impurities. The iron-based alloy is obtained by a first heat treatment for applying a solid so...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SUGAWARA, TAKESHI, YAMADA, NORIYUKI, ASAMI, MAKOTO
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:An iron-based alloy comprises 1.5 to 2.5 wt% of C, 0.25 to 4.75 wt% of Ni, and W and V in quantities surrounded by the line L as shown in Fig. 1 of the attached drawings with a balance of Fe and inevitable impurities. The iron-based alloy is obtained by a first heat treatment for applying a solid solution treatment by rapidly cooling the iron-based alloy from a temperature of an austenite forming temperature or more to consequently obtain a mixed matrix comprising a base matrix of martensite and remaining austenite phases and a non-molten carbide, and a second heat treatment for cooling the iron-based alloy after precipitating an MC type carbide within an eutectoid transformation temperature range to consequently precipitate a low carbon content austenite phase.