HIGH-STRENGTH POLYAMIDE FIBER

To provide a polyamide fiber such as polyhexa- methylene adipamide fiber having high tenacity and excellent tenacity retention after vulcanization and GY fatigue life. This fiber is a high tenacity polyamide fiber, preferably a polyhexamethylene adipamide fiber comprising at least 95$ by mole of hex...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TUDUKI, MICHIKANE, OKANO, RYOJI, NAGAHARA, HIDEO, SAITO, ISOO
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a polyamide fiber such as polyhexa- methylene adipamide fiber having high tenacity and excellent tenacity retention after vulcanization and GY fatigue life. This fiber is a high tenacity polyamide fiber, preferably a polyhexamethylene adipamide fiber comprising at least 95$ by mole of hexamethylene adipamide units and having a sulfuric acid relative viscosity of at least 3.0, said polyamide fiber satisfying the requirements: (a) differential birefringence .delta..DELTA.n ~ -5 .times. 10-3 to 0 .times. 10-3, (b) long period (Dm) in the direction of fiber axis: Dm ~ 105 A, and long period (De) in the radial direction of fiber: De = 90 to 130 A, (c) main dispersion peak temperature (T.alpha.) in mechanical loss tangent (tan.delta.) curve as obtained by viscoelastic measurement: T.alpha. ~ 125.degree.C, and preferably further satisfying the requirements: (d) birefringence .DELTA.n ~ 60 .times. 10-3, (e) crystal orientation function fc ~ 0.88, and (f) amorphous orientation function fa = 0.70 to 0.85.