METHOD FOR PRODUCING SINTERED SILICON CARBIDE ARTICLES

Production of sintered silicon carbide articles by mixing a tar pitch in an amount to provide 4.2-6 parts by weight of carbon after being carbonized and boron or a boron compound in an amount corresponding to 0.03 - 0.15 parts by weight of boron content as densification aids with 100 parts by weight...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MOURI, MASAHIDE, YAMADA, KOICHI, NOMURA, YOSHISABURO
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Production of sintered silicon carbide articles by mixing a tar pitch in an amount to provide 4.2-6 parts by weight of carbon after being carbonized and boron or a boron compound in an amount corresponding to 0.03 - 0.15 parts by weight of boron content as densification aids with 100 parts by weight of a finely divided silicon carbide powder, shaping the resulting mixture, and sintering the shaped article in an inert atmosphere at a temperature of from 1900 to 2300.degree.C. The articles can be produced with increased sintered density and mechanical strength.