HYDROMETALLURGICAL PROCESS FOR EXTRACTING ZINC

GC78 In a process according to the present invention zinc is extracted from zinc sulphide containing ores using an aqueous sulphuric acid leaching liquor containing as primary oxidising agent either hydrogen peroxide or monoperoxosulphuric acid. Preferably the leaching is effected at a temperature o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WHITTEMORE, ROBERT G, COVINGTON, JAMES W
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:GC78 In a process according to the present invention zinc is extracted from zinc sulphide containing ores using an aqueous sulphuric acid leaching liquor containing as primary oxidising agent either hydrogen peroxide or monoperoxosulphuric acid. Preferably the leaching is effected at a temperature of at least 70.degree.C and especially from 90 to 100.degree.C. The acidity of the leach liquor is preferably maintained at below pH 1.5 and especially to produce a final pH below pH 1.0. Preferably the oxident is introduced into the leaching solution progressively, maintaining its electrochemical potential at 450 mV or higher. The invention also provides a method for preferentially leaching zinc from an ore containing both sphalente and chalcopyrite.