METHOD OF MAKING IRON POWDER

Iron oxide particles are made by spray calcination and the oxide is reduced at least substantially in CO at temperatures between 800.degree. and 1000.degree. C The oxide is heat-treated prior to calcination or Cao is added to enhance formation of iron fibers. The reducing atmosphere may in parts inc...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GREBE, KLAUS, HEWING, JOSEF, DAUTZENBERG, NORBERT, DE HAAS, HANS
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Iron oxide particles are made by spray calcination and the oxide is reduced at least substantially in CO at temperatures between 800.degree. and 1000.degree. C The oxide is heat-treated prior to calcination or Cao is added to enhance formation of iron fibers. The reducing atmosphere may in parts include hydrogren or the last phase of reduction is carried out in hydrogen. The iron cake is cooled and broken up in a grinder. The resulting powder has low bulk density due to a fiber-like, nonporous consistency of its particles. Grinding may continue to increase bulk density.